Processing Properties Metric English Comments
Adapter Temperature 180 - 200 °C
356 - 392 °F
Petroquimica Triunfo Trilene® TS 8056 LLDPE-C8 and LDPE Blend
The Trilene TS 8056 product is a blend with a high ratio of linear low-density polyethylene - octene comonomer (LLDPE-C8) with low-density polyethylene (LDPE) with elevated processability, ensuring ..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1214 AC Ethylene and 14% Methyl Acrylate Copolymer  (discontinued **)
Elvaloy® 1214 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Adapter Temperature 180 °C
356 °F
Blow Film
DuPont Appeel® LSR11N704 Lidding Sealant Resin  (discontinued **)
Appeel® 11N704 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide very strong peelable seal..
Adapter Temperature 180 - 195 °C
356 - 383 °F
Petroquimica Triunfo Trithene® TX 3003 LDPE - Shrink Wrap Film
The Trithene® TX 3003 resin is a low-density polyethylene (LDPE) with high molecular weight, presenting excellent mechanical properties. The product provided elevated gloss and transparency, adding..
Adapter Temperature 180 - 205 °C
356 - 401 °F
Extrusion
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade
High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman
Adapter Temperature 180 - 205 °C
356 - 401 °F
Extrusion
Huntsman IROGRAN® A 85 D 5001 DP TPU-Polyester
Introduction: IROGRAN A 85 D 5001 DP is a antistatic, polyester based thermoplastic polyurethane intended for extrusion applications and injection molding. IROGRAN A 85 D 5001 DP is part of the HUNT..
Adapter Temperature 180 - 200 °C
356 - 392 °F
Extrusion Molding
LG Chemical KEYFLEX BT 10288D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 180 - 200 °C
356 - 392 °F
Extrusion Molding
LG Chemical KEYFLEX BT 3140D Ester Type TPE
Description: Injection Molding, TPC-ET, Specialty, Low Melting Temperature, Low ModulusApplication: Masterbatch Carrier, Cable Compound BaseCAS: 37282-12-5Information provided by LG Chemical
Adapter Temperature 180 °C
356 °F
Ideal, Extrusion Blow Molding
LG Chemical LUTENE-H BE0400 HDPE
Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con..
Adapter Temperature 180 °C
356 °F
Extrusion
Huntsman IROGRAN® A 80 P 4699L Ether-Based TPU-For Cable Industry
Introduction: IROGRAN A 80 P 4699 L is a high performance polyether based thermoplastic polyurethane intended for extrusion and injection mold applications. IROGRAN A 80 P 4699 L is part of the HUNT..
Adapter Temperature 180 °C
356 °F
Taiwan PU Corporation TPU-C75 General Grade, Calender Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1209 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1209 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1224 AC Ethylene and 24% Methyl Acrylate Copolymer
Elvaloy® 1224 AC is intended for extrusion, coextrusion, compounding and injection molding. Elvaloy® 1224 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent ..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1609 AC Ethylene and 9% Methyl Acrylate Copolymer
Elvaloy® 1609 AC is intended for film coextrusion and injection molding. It can be recommended in film applications where softness, flexibility and excellent sealing properties are needed.Elvaloy®..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer
Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 2116 AC Ethylene and 16% Ethyl Acrylate Copolymer
Elvaloy® 2116 AC is intended for profile and tube extrusion. Its good chemical resistance, low temperature toughness and good flex life make it outstanding for specialty tubing. The material also..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 3117 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3117 AC is intended for coextrusion and compounding. Due to its high melt flow rate, it is used also in extrusion coating. Elvaloy® 3117 AC is soft, flexible and has good adhesion to va..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 3717 AC Ethylene and 17% Butyl Acrylate Copolymer
Elvaloy® 3717 AC can be used for coextrusion, compounding and injection molding. In coextrusion, it can be used to improve sealing; in compounding, to improve low temperature and impact properties..
Adapter Temperature 180 °C
356 °F
5, Extrusion
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane
Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H..
Adapter Temperature 180 °C
356 °F
Blow Film
DuPont Appeel® LSR11D554 Lidding Sealant Resin
Appeel® LSR11D554 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals to poly..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1218 AC Ethylene and 18% Methyl Acrylate Copolymer
Elvaloy® 1218 AC is intended for coextrusion, compounding and injection molding. Elvaloy® 1218 AC has good adhesion to various substrates (OPA, OPP, paperboard, etc.), gives excellent sealing pro..
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D875 Ethylene Acrylate
Appeel® 20D875 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide strong peelable seals over a broad tempe..
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 22D843 Ethylene Acrylate
DuPont™ Appeel® 22D843 is a polypropylene modified ethylene acrylate resin designed to function as a masterbatch to achieve peelability in polypropylene based sealant layers. It provides peelable ..
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 72D727 Sealing Resin
DuPont™ Appeel® 72D727 is a blown or cast film resin designed to be a sealing layer to film or sheet lidding applications. It provides a peelable seal to a number of materials including HDPE, LLDP..
Adapter Temperature 180 °C
356 °F
Blown Film Coextrusion
DuPont™ Appeel® 20D784 Ethylene Acrylate
Appeel® 20D784 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperature ..
Adapter Temperature 180 - 195 °C
356 - 383 °F
Petroquimica Triunfo Trithene® TS 3003 LDPE - Film Grade
The Trithene® TS 3003 resin is a low-density, high molecular weight polyethylene that offers high mechanical strength and excellent optical properties. The product shows high modulus of elasticity,..
Adapter Temperature 180 - 216 °C
356 - 421 °F
Average value: 193 °C Grade Count:24
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer  (discontinued **)
Elvaloy® 1126 AC is intended for coextrusion and molding. It can be recommended for blow molding of parts requiring permanent flexibility, stress cracking resistance and softness. Excellent fill..
Adapter Temperature 180 °C
356 °F
Blown film
DuPont Elvaloy® 3108 AC Ethylene and 7% Butyl Acrylate Copolymer  (discontinued **)
Elvaloy® 3108 AC contains antioxidant, slip and antiblock additives.Elvaloy® 3108 AC is developed to give films with good sealing properties, impact strength at lower temperature, and low shrinkag..