| Category | Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade |
| Manufacturer | |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.04 - 1.27 g/cc | 0.0376 - 0.0459 lb/in³ | Average value: 1.14 g/cc Grade Count:122 |
| Water Absorption | 1.08 - 1.50 % | 1.08 - 1.50 % | Average value: 1.36 % Grade Count:3 |
| Water Vapor Transmission | 420 - 9000 g/m²/day | 27.0 - 580 g/100 in²/day | Average value: 3770 g/m²/day Grade Count:7 |
| 6000 - 9500 g/m²/day <br>@Temperature 38.0 - 38.0 °C |
386 - 612 g/100 in²/day <br>@Temperature 100 - 100 °F |
Average value: 7750 g/m²/day Grade Count:1 | |
| Maximum Moisture Content | 0.0200 - 0.0500 | 0.0200 - 0.0500 | Average value: 0.0260 Grade Count:10 |
| Linear Mold Shrinkage | 0.00500 - 0.0450 cm/cm | 0.00500 - 0.0450 in/in | Average value: 0.0123 cm/cm Grade Count:15 |
| Linear Mold Shrinkage, Transverse | 0.000 - 0.0200 cm/cm | 0.000 - 0.0200 in/in | Average value: 0.00800 cm/cm Grade Count:7 |
| Melt Flow | 10.0 - 54.0 g/10 min | 10.0 - 54.0 g/10 min | Average value: 15.5 g/10 min Grade Count:16 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 25.0 - 101 | 25.0 - 101 | Average value: 83.1 Grade Count:119 |
| Hardness, Shore D | 22.0 - 83.0 | 22.0 - 83.0 | Average value: 54.5 Grade Count:33 |
| Tensile Strength, Ultimate | 0.800 - 68.9 MPa | 116 - 10000 psi | Average value: 26.1 MPa Grade Count:120 |
| 10.3421 - 13.7895 MPa <br>@Temperature 100 - 121 °C |
1500.00 - 2000.00 psi <br>@Temperature 212 - 250 °F |
Average value: 12.0 MPa Grade Count:1 | |
| 10.3421 - 13.7895 MPa <br>@Time 605000 - 605000 sec |
1500.00 - 2000.00 psi <br>@Time 168 - 168 hour |
Average value: 12.0 MPa Grade Count:1 | |
| Tensile Strength, Yield | 1.80 - 70.0 MPa | 261 - 10200 psi | Average value: 14.2 MPa Grade Count:104 |
| Elongation at Break | 77.0 - 1000 % | 77.0 - 1000 % | Average value: 573 % Grade Count:126 |
| 270 - 324 % <br>@Temperature 100 - 121 °C |
270 - 324 % <br>@Temperature 212 - 250 °F |
Average value: 294 % Grade Count:1 | |
| 270 - 324 % <br>@Time 605000 - 605000 sec |
270 - 324 % <br>@Time 168 - 168 hour |
Average value: 294 % Grade Count:1 | |
| Elongation at Yield | 320 - 850 % | 320 - 850 % | Average value: 528 % Grade Count:18 |
| Modulus of Elasticity | 0.00670 - 0.129 GPa | 0.972 - 18.7 ksi | Average value: 0.0324 GPa Grade Count:6 |
| Flexural Yield Strength | 1.55 - 75.2 MPa | 225 - 10900 psi | Average value: 27.6 MPa Grade Count:3 |
| Flexural Modulus | 0.0162 - 1.99 GPa | 2.35 - 289 ksi | Average value: 0.289 GPa Grade Count:16 |
| Resilience | 30.0 - 65.0 | 30.0 - 65.0 | Average value: 46.9 Grade Count:18 |
| Rebound | 1.00 - 72.0 % | 1.00 - 72.0 % | Average value: 41.2 % Grade Count:6 |
| Izod Impact, Notched (ISO) | 7.50 - 10.5 kJ/m² <br>@Temperature -20.0 - -20.0 °C |
3.57 - 5.00 ft-lb/in² <br>@Temperature -4.00 - -4.00 °F |
Average value: 8.82 kJ/m² Grade Count:4 |
| Charpy Impact, Notched | 5.00 - 1000 J/cm² | 23.8 - 4760 ft-lb/in² | Average value: 7.00 J/cm² Grade Count:13 |
| 0.300 - 999.9 J/cm² <br>@Temperature -30.0 - -30.0 °C |
1.43 - 4759 ft-lb/in² <br>@Temperature -22.0 - -22.0 °F |
Average value: 7.95 J/cm² Grade Count:13 | |
| Coefficient of Friction | 0.0110 - 7.40 | 0.0110 - 7.40 | Average value: 2.96 Grade Count:5 |
| Tear Strength | 7.01 - 1050 kN/m | 40.0 - 5990 pli | Average value: 147 kN/m Grade Count:115 |
| Graves Tear Strength | 47.3 - 245 kN/m | 270 - 1400 pli | Average value: 104 kN/m Grade Count:9 |
| K Factor (Wear Factor) | 40.0 - 100 | 40.0 - 100 | Average value: 63.1 Grade Count:18 |
| Taber Abrasion, mg/1000 Cycles | 5.00 - 340 | 5.00 - 340 | Average value: 51.1 Grade Count:45 |
| Compression Set | 1.00 - 70.0 % | 1.00 - 70.0 % | Average value: 24.1 % Grade Count:60 |
| 23.0 - 100 % <br>@Temperature 70.0 - 70.0 °C |
23.0 - 100 % <br>@Temperature 158 - 158 °F |
Average value: 42.8 % Grade Count:43 | |
| 22.9 - 95.0 % <br>@Temperature 70.0 - 70.0 °C |
22.9 - 95.0 % <br>@Temperature 158 - 158 °F |
Average value: 42.8 % Grade Count:28 | |
| 22.9 - 95.0 % <br>@Time 79200 - 86400 sec |
22.9 - 95.0 % <br>@Time 22.0 - 24.0 hour |
Average value: 42.8 % Grade Count:28 | |
| Tensile Set | 5.60 - 53.0 % | 5.60 - 53.0 % | Average value: 15.4 % Grade Count:7 |
| Torsional Stiffness | 22.0 - 472 MPa | 3190 - 68500 psi | Average value: 181 MPa Grade Count:5 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 86.4 - 179 µm/m-°C | 48.0 - 99.6 µin/in-°F | Average value: 139 µm/m-°C Grade Count:3 |
| Melting Point | 118 - 218 °C | 244 - 424 °F | Average value: 156 °C Grade Count:23 |
| Vicat Softening Point | 46.0 - 152 °C | 115 - 306 °F | Average value: 96.0 °C Grade Count:35 |
| Softening Point | 110 - 166 °C | 230 - 330 °F | Average value: 134 °C Grade Count:3 |
| Brittleness Temperature | -70.0 - -68.0 °C | -94.0 - -90.4 °F | Average value: -68.5 °C Grade Count:4 |
| Glass Transition Temp, Tg | -76.0 - -10.0 °C | -105 - 14.0 °F | Average value: -42.9 °C Grade Count:43 |
| Flammability, UL94 | V-2 - V-0 | V-2 - V-0 | Grade Count:14 |
| Oxygen Index | 21.0 - 38.0 % | 21.0 - 38.0 % | Average value: 31.8 % Grade Count:4 |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.49 - 1.50 | 1.49 - 1.50 | Average value: 1.49 Grade Count:4 |
| Haze | 0.000 - 0.300 % | 0.000 - 0.300 % | Average value: 0.225 % Grade Count:4 |
| Yellow Index | 1.00 % | 1.00 % | Average value: 1.00 % Grade Count:4 |
| Transmission, Visible | 85.0 - 95.0 % | 85.0 - 95.0 % | Average value: 90.0 % Grade Count:4 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.70 - 6.70 | 3.70 - 6.70 | Average value: 5.16 Grade Count:4 |
| Dielectric Strength | 14.3 - 15.4 kV/mm | 363 - 392 kV/in | Average value: 15.0 kV/mm Grade Count:3 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Processing Temperature | 160 - 240 °C | 320 - 464 °F | Average value: 197 °C Grade Count:27 |
| Nozzle Temperature | 175 - 220 °C | 347 - 428 °F | Average value: 205 °C Grade Count:6 |
| Adapter Temperature | 180 - 216 °C | 356 - 421 °F | Average value: 193 °C Grade Count:24 |
| Die Temperature | 170 - 365 °C | 338 - 689 °F | Average value: 194 °C Grade Count:33 |
| Melt Temperature | 149 - 240 °C | 300 - 464 °F | Average value: 184 °C Grade Count:40 |
| Mold Temperature | 10.0 - 70.0 °C | 50.0 - 158 °F | Average value: 38.9 °C Grade Count:18 |
| Drying Temperature | 70.0 - 180 °C | 158 - 356 °F | Average value: 98.7 °C Grade Count:14 |
| Moisture Content | 0.100 % | 0.100 % | Average value: 0.100 % Grade Count:6 |
| Dew Point | -40.0 - -5.00 °C | -40.0 - 23.0 °F | Average value: -35.9 °C Grade Count:11 |
| Injection Pressure | 8.27 - 138 MPa | 1200 - 20000 psi | Average value: 34.8 MPa Grade Count:4 |