DuPont Appeel® LSR11D554 Lidding Sealant Resin

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Appeel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Appeel® LSR11D554 Lidding Sealant Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Appeel® LSR11D554 is a modified ethylene vinyl acetate copolymer resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals to polypropylene, polystyrene and polystyrene foam and is available in pellet form for use in conventional extrusion or coextrusion equipment designed to process polyethylene resins. Information provided by DuPont™
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
ASTM D792
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Thermal Properties Metric English Comments
Melting Point 95.0 °C
203 °F
DSC; ASTM D3418
Vicat Softening Point 72.0 °C
162 °F
ASTM D1525
Processing Properties Metric English Comments
Rear Barrel Temperature 140 °C
284 °F
Blow Film
160 °C
320 °F
Extrusion Coating
Middle Barrel Temperature 150 °C
302 °F
Blow Film
220 °C
428 °F
Extrusion Coating
Front Barrel Temperature 160 °C
320 °F
Blow Film
234 °C
453 °F
Extrusion Coating
Adapter Temperature 180 °C
356 °F
Blow Film
234 °C
453 °F
Extrusion Coating
Die Temperature 180 °C
356 °F
Blow Film
235 °C
455 °F
Extrusion Coating