Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear, Parallel to Flow = 21.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® HPN 9233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron HPN 9233G is a 33% glass reinforced polyamide 6 injection molding compound combining exceptional strength, stiffness and high temperature performance with excellent surface aesthetics. It is..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP 5CL23 FP-V (PVDF)
LNP* LUBRICOMP* 5CL23 is a compound based on PVDF resin containing 15% Carbon Fiber, 10% PTFE. Added features include: Wear Resistant.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
Idemitsu Kosan Xarec® WA 212 SPS, 30% Glass Filled
Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
Idemitsu Kosan Xarec® WA 212LG SPS, 30% Glass Filled
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP QCL34 PA6.10
LNP* LUBRICOMP* QCL34 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp RFL38 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RFL38 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA
LNP* LUBRICOMP* UFL36AS is a Polyphthalamide (PPA) base resin containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Heat Stabilized, Wear Resistant.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON AE008XXY ABS
LNP* STAT-KON* AE008XXY is a compound based on ABS resin containing 40% Carbon Fiber. Added feature of this material ia: Electrically Conductive.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS
LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP STAT-KON WEF42I PBT
LNP* STAT-KON* WEF42I is a compound based on PBT resin containing 10% Carbon Fiber, 20% Glass Fiber. Added features of this grade include: High Impact, Electrically Conductive.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP WX05502 Polyester Elastomer
LNP THERMOCOMP* WX05502 is a compound based on Polyester, TP resin containing Flame Retardant, Glass Fiber, Mineral. Added features of this material include: Flame Retardant.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Inf..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Sumitomo Bakelite North America 52-70-70-VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Conforms with the requirements of ASTM D5948 Type..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Sumitomo Bakelite North America 73-70-70 C-P /73-70-70 VO-P Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG-F.I..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ASTM E-831
Sumitomo Bakelite North America RX® 1-520/RX® 1310 Short-Glass Reinforced Diallyl Phthalate
Short glass fiber reinforced, non-flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type SDG.Information provided by Vyncolit, a Sumitomo Bak Group..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP VERTON RV00AESC PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AESC is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, Heat Stabilized.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -40.0 - 23.0 °C
11.7 µin/in-°F

@Temperature -40.0 - 73.4 °F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 77G43L BK031 Nylon 612  (Unverified Data**)
43% Glass Reinforced Polyamide 612Information provided by DuPont Performance Polymers
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide AG8 PA66, 40% Glass Fiber Reinforced, Injection Molding
Staramide AG8 is a 40% Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG7H PA6, 35% Glass Fiber Filled, Heat Stabilized, Injection Molded
Staramide BG7H is a Heat Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded
Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Starflam AFR470X2 PA66, 35% Glass Filled, Injection Molded
AFR470X2 is a Red Phosphorous, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
11.7 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide PF007 PA6, 35% Glass Fiber Filled, Injection Molded
Staramide PF007 is a 35% Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
CTE, linear, Parallel to Flow 21.0 µm/m-°C
11.7 µin/in-°F
ISO 11359
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
Ultramid 8233G HS is a heat stabilized, 33% glass fiber reinforced nylon 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also..
CTE, linear, Parallel to Flow 21.0 - 23.0 µm/m-°C

@Temperature 23.0 - 80.0 °C
11.7 - 12.8 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 11359-1/-2
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Dry)
Description: Flame retardant without halogens and red phosphorus, 25% glass fiber reinforced injection-molding grade; light colorable; outstanding mechanical and electrical properties.Information pr..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ISO data
BASF Capron® 8233G 33% Glass-Filled Nylon 6 (Dry)  (discontinued **)
Capron 8233G is a 33% glass fiber reinforced polyamide 6 molding compound offering excellent strength, stiffness, high temperature performance and dimensional stability. It is also available in he..
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
11.7 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP DX07408 PC
LNP* THERMOCOMP* DX07408 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: UL Rated.
Copyright © lookpolymers.com All Rights Reserved