Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate

Category Polymer , Thermoset , Diallyl Phthalate (DAP) , Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled , Filled/Reinforced Thermoset
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America 52-01 Short-Glass Reinforced Diallyl Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SDG.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.93 g/cc
0.0697 lb/in³
ASTM D792
Apparent Bulk Density 0.750 g/cc
0.0271 lb/in³
Water Absorption 0.25 %
0.25 %
48 hours, 50°C. ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
Compression Molding. ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 69.0 MPa
10000 psi
ASTM D638
Flexural Yield Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Compressive Yield Strength 130 MPa
18900 psi
ASTM D695
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.0 µm/m-°C

@Temperature 20.0 °C
11.7 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Thermal Conductivity 0.281 W/m-K
1.95 BTU-in/hr-ft²-°F
ASTM F433
Maximum Service Temperature, Air 130 °C
266 °F
UL temperature Index, UL 746B
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
401 °F
as molded; ASTM D648
UL RTI, Electrical 130 °C
266 °F
UL temperature Index, UL 746B
UL RTI, Mechanical with Impact 130 °C
266 °F
UL temperature Index, UL 746B
UL RTI, Mechanical without Impact 130 °C
266 °F
UL temperature Index, UL 746B
Oxygen Index 26 %
26 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.5

@Frequency 1e+6 Hz
3.5

@Frequency 1e+6 Hz
Wet
4.0

@Frequency 1000 Hz
4.0

@Frequency 1000 Hz
Wet
Dielectric Strength 13.8 kV/mm
351 kV/in
Wet, step-by-step. ASTM D149
Dissipation Factor 0.010

@Frequency 1000 Hz
0.010

@Frequency 1000 Hz
Wet; ASTM D150
0.016

@Frequency 1e+6 Hz
0.016

@Frequency 1e+6 Hz
Wet; ASTM D150
Arc Resistance 150 sec
150 sec
ASTM D495
Comparative Tracking Index >= 600 V
>= 600 V
UL746A, ASTM D3638
Processing Properties Metric English Comments