| Category | Polymer , Thermoplastic , Polycarbonate (PC) |
| Manufacturer | SABIC Innovative Plastics (GE Plastics) |
| Trade Name | LNP STAT-KON |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | SABIC Innovative Plastics LNP STAT-KON DE0049F PC.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.33 g/cc | 0.0480 lb/in³ | ASTM D792 |
| 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 | |
| Moisture Absorption | 0.130 % | 0.130 % | 50% RH, 24 hrs; ASTM D570 |
| 0.180 % | 0.180 % | 23°C / 50% RH; ISO 62 | |
| Linear Mold Shrinkage, Flow | 0.0070 - 0.010 cm/cm <br>@Time 86400 sec |
0.0070 - 0.010 in/in <br>@Time 24.0 hour |
ASTM D955 |
| Linear Mold Shrinkage, Transverse | 0.0040 - 0.0070 cm/cm <br>@Time 86400 sec |
0.0040 - 0.0070 in/in <br>@Time 24.0 hour |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 134 MPa | 19400 psi | 5 mm/min; ISO 527 |
| 137 MPa | 19900 psi | Type I, 5 mm/min; ASTM D638 | |
| Tensile Strength, Yield | 134 MPa | 19400 psi | 5 mm/min; ISO 527 |
| 137 MPa | 19900 psi | Type I, 5 mm/min; ASTM D638 | |
| Elongation at Break | 1.6 % | 1.6 % | 5 mm/min; ISO 527 |
| 1.9 % | 1.9 % | Type I, 5 mm/min; ASTM D638 | |
| 166 % | 166 % | Flexural Strain, break, 2 mm/min; ISO 178 | |
| Elongation at Yield | 1.6 % | 1.6 % | 5 mm/min; ISO 527 |
| 1.9 % | 1.9 % | Type I, 5 mm/min; ASTM D638 | |
| Tensile Modulus | 13.42 GPa | 1946 ksi | 50 mm/min; ASTM D638 |
| 14.97 GPa | 2171 ksi | 1 mm/min; ISO 527 | |
| Flexural Strength | 190 MPa | 27600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
| Flexural Yield Strength | 166 MPa | 24100 psi | 2 mm/min; ISO 178 |
| Flexural Modulus | 11.55 GPa | 1675 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
| 11.65 GPa | 1690 ksi | 2 mm/min; ISO 178 | |
| Izod Impact, Notched | 0.470 J/cm | 0.881 ft-lb/in | ASTM D256 |
| Izod Impact, Unnotched | 4.88 J/cm | 9.14 ft-lb/in | ASTM D4812 |
| Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
| Izod Impact, Unnotched (ISO) | 29.0 kJ/m² | 13.8 ft-lb/in² | 80*10*4; ISO 180/1U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 1.23 µm/m-°C <br>@Temperature 23.0 - 60.0 °C |
0.683 µin/in-°F <br>@Temperature 73.4 - 140 °F |
ISO 11359-2 |
| 1.23 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
0.683 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 | |
| CTE, linear, Transverse to Flow | 6.79 µm/m-°C <br>@Temperature 23.0 - 60.0 °C |
3.77 µin/in-°F <br>@Temperature 73.4 - 140 °F |
ISO 11359-2 |
| 6.79 µm/m-°C <br>@Temperature -40.0 - 40.0 °C |
3.77 µin/in-°F <br>@Temperature -40.0 - 104 °F |
ASTM E 831 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 148 °C | 298 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
| 146 °C <br>@Thickness 3.20 mm |
295 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 | |
| Deflection Temperature at 1.8 MPa (264 psi) | 144 °C | 291 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
| 143 °C <br>@Thickness 3.20 mm |
289 °F <br>@Thickness 0.126 in |
unannealed; ASTM D648 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Surface Resistance | 10 - 1000 ohm | 10 - 1000 ohm | ASTM D257 |