| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ISO 2577 |
|
PolyOne Edgetek® QT-30GF/000 Natural Syndiotactic Polystyrene (SPS)
Information provided by PolyOne
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ASTM D955 |
|
PolyOne Nymax™ NM 6600-44GF0001 White Polyamide 66 (Nylon 66)
The Nymax® GMF 1200 Series of compounds are based upon nylon 6/6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part per..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0070
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0070
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical LUMID GP2430A(W) PA6+GF43%, General Purpose
Feature: Injection Molding, PA6+GF43%, General PurposeApplication: Automotive (Air Intake Manifold, Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0060
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0060
in/in @Thickness 0.126 in |
ASTM D955 |
|
LG Chemical Lupox® LW5402A PBT+PC+GF40%
Description: Injection Molding, PBT+PC+GF40%, Low Warpage, High GlossApplication: E&E, Automotive (Bobbin, Switch)CAS No. 9010-86-0, 65997-17-3, 24968-12-5 and 103598-77-2Information provided by LG ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | ASTM D995 |
|
Kotec Carbotex KG-20F10 Polycarbonate, Wear Resistant, 20% Glass Fiber Reinforced
Features: Glass fiber 20% reinforced, Mold release, Translucent, Dimensional stability, Non-frictionApplications: OA equipment, Communications, Precision parts, Machineries, E & E partsInformation p..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm @Thickness 3.17 mm |
0.0030
in/in @Thickness 0.125 in |
1/8" Section |
|
Lucent Polymers GPP-140 Polypropylene Homopolymer, 40% Glass Fiber Reinforced, Chemically Coupled
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
|
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm @Temperature 80.0 °C |
0.0030
in/in @Temperature 176 °F |
60x60x2 mm; ISO 294-4 |
|
Gromax BFG30-AH00B3 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0060 cm/cm | 0.0030 - 0.0060 in/in | |
|
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | |
|
LATI Latigloss 66 H2 G/60 PA 66, 60% Glass Fiber Reinforced, Heat Stabilized
Product with high mechanical properties and exceptional surface finish based on Polyamide 66 (PA66). Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0050
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Europe-Africa-Middle East)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0050
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Ultem 2200N PEI (Asia Pacific)
20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0040
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0040
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics ULTEM 2312 PEI
30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0050
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Ultem ATX202R PEI+PCE (Europe-Africa-Middle East)
20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | on tensile bar; SABIC Method |
|
SABIC Innovative Plastics Ultem PW2200 PEI (Europe-Africa-Middle East)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water
applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0070 cm/cm | 0.0030 - 0.0070 in/in | on Tensile Bar; SABIC Method |
|
SABIC Innovative Plastics Valox® 4022 PBT (Europe-Africa-Middle East)
VALOX 4022 is a 20% high strength glass fibre reinforced PBT injection moulding resin, with improved mechanical properties. Applications : Spotlights, appliance housings and handles.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm @Time 86400 sec |
0.0030
in/in @Time 24.0 hour |
ISO 294 |
|
SABIC Innovative Plastics LNP STAT-KON SE002Z PA 12 (Asia Pacific)
LNP* Stat-kon* SE002Z is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0060
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0060
in/in @Thickness 0.126 in |
ASTM D955 |
|
Samsung Cheil Industries Starex® SF-0950S MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm @Time 86400 sec |
0.0030
in/in @Time 24.0 hour |
ASTM D955 |
|
SABIC Innovative Plastics LNP THERMOTUF PF008IR PA 6
LNP* Thermotuf* PF008IR is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact, Mold Release.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4, 2577 |
|
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23
Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**)
35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo..
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
33% Glass Reinforced Polyamide 612 with Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | DAM; ISO 294-4 2577 |
|
DuPont Performance Polymers Zytel® PLS 95G40DH1T BK261 Nylon 6
(Unverified Data**)
40% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G40DH1T is a 40% GR impact modified PA made with SHIELD technology its superior heatInformation provided by DuPont Performance Polymers
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0040 cm/cm | 0.0030 - 0.0040 in/in | on Tensile Bar; ISO 294 |
|
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded
BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0050
cm/cm @Thickness 4.00 mm |
0.0030
-
0.0050
in/in @Thickness 0.157 in |
E2P method |
|
Eurostar Starflam RX06082 PA66/6, Glass Fiber Filled, Flame Retardant, Injection Molded
Staramide RX06082 is a Halogen Free and Red Phosphorous Free, flame Retardant, Glass Fiber Reinforced Polyamide 66/Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 - 0.0050 cm/cm | 0.0030 - 0.0050 in/in | ASTM D955 |
|
BLUESTAR LXS 314 G20 PPE-HIPS, 20% Glass Filled
Typical Applications: Water industrial partsInformation provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Linear Mold Shrinkage, Flow | 0.0030 cm/cm | 0.0030 in/in | ISO 294-4 |
|
Solvay Specialty Polymers Amodel® A-6625 HS BK324 Polyphthalamide, 25% carbon/glass fiber, ESD grade
(discont
Amodel A-6625 HS BK324 is a 25% carbon and glass-fiber-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This ..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
-
0.0040
cm/cm @Thickness 3.20 mm |
0.0030
-
0.0040
in/in @Thickness 0.126 in |
SABIC Method |
|
SABIC Innovative Plastics Lexan® HFD4471 PC
Lexan* HFD4471 is a 10% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4417 has enhanced mold release, impact ductili..
|
|||
| Linear Mold Shrinkage, Flow |
0.0030
cm/cm @Thickness 3.17 mm |
0.0030
in/in @Thickness 0.125 in |
ASTM D955 |
|
Techmer ES HiFill FR® PA6/6 GF25 FR NAT005 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized, High Flow and Lubri..
|
|||