Material Notes:
LTHA injection molding homopolymerLTHA - FINA 3429 is engineered with an LTHA additive system that gives excellent leach resistance in hot/wet environments that contain bleach and laundry detergents.UL Rating - FINA 3429 has a UL rating at 120oC (248oF)FDA - FINA 3429 complies with all applicable FDA regulations for food contact applications.Recommended Applications - FINA 3429 is recommended for appliance parts and is particularly suited for parts that are exposed to a hot/wet environment such as: washing machine, dishwasher and coffee machine parts.Processing - FINA 3429 resin processes on conventional injection molding equipment with typical melt temperatures of 390-450°F (200-232°C)Data provided by the manufacturer, Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D1505
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238L
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM D288A
Tensile Strength, Ultimate 33.1 MPa
4800 psi
ASTM D638
Elongation at Break 8.0 %
8.0 %
ASTM D638
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.599 ft-lb/in
ASTM D256A
Izod Impact, Unnotched 12.8 J/cm
24.0 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Melting Point 165 °C
329 °F
DSC
Maximum Service Temperature, Air 120 °C
248 °F
UL Rating
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 200 - 232 °C
392 - 450 °F
Injection