Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D-4812 |
PlastiComp Velocity® LGF60-PA6 High Flow Nylon 6, 60% Long Glass Fiber This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 12.8 J/cm @Thickness 3.17 mm |
24.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PEI BK Availability: North AmericaForms: PelletsAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 12.8 J/cm @Thickness 3.17 mm |
24.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PEI HF BK Availability: North AmericaForms: PelletsFeatures: High FlowAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 12.8 J/cm @Thickness 3.17 mm |
24.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PEI TX5 LE Availability: North AmericaForms: PelletsAdditive: PTFE LubricantFeatures: Low Extractables and LubricatedInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 12.8 J/cm @Thickness 3.17 mm |
24.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES HiFill® PEI/C GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Izod Impact, Unnotched | 12.8 J/cm @Thickness 3.17 mm |
24.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Luriblend® PA6/6 GF40 TL10 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 40% Filler by WeightAdditive: Heat Stabilizer and PTFE Lubricant(10%)Features: Lubricated and Heat StabilizedInformation p.. |
|||
Izod Impact, Unnotched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66 LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Izod Impact, Unnotched | 12.8 J/cm | 24.0 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® RMC-20 20% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Izod Impact, Unnotched | 12.8 J/cm | 24.0 ft-lb/in | At 73°F; ASTM D256 |
Plastics Group Polifil® RMC-20V 20% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar.. |
|||
Izod Impact, Unnotched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D256 |
Westlake Plastics Zelux® 40% GF Polycarbonate 40% Glass Filled Zelux polycarbonate is a transparent engineering plastic with excellent dimensional stability and good mechanical and electrical properties. It is used for structural applications when clarity and .. |
|||
Izod Impact, Unnotched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D256A |
Total PPH 3429 Polypropylene, Injection Molding Grade LTHA injection molding homopolymerLTHA - FINA 3429 is engineered with an LTHA additive system that gives excellent leach resistance in hot/wet environments that contain bleach and laundry detergents.. |
|||
Izod Impact, Unnotched | 12.8 J/cm | 24.0 ft-lb/in | ASTM D4812 |
Premix Premi-Glas® 1285VE 1285 VE Glass Reinforced Vinyl Ester SMC
(discontinued **) Description: Premi-Glas® 1285 VE is a glass reinforced vinyl ester sheet molding compound designed for automotive under the hood applications. Key features and benefits: Designed for compression mo.. |