Polymer Property : Melt Flow = 4.5 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Plaskolite West Optix® CA - 927 High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Melt Flow 4.5 g/10 min
4.5 g/10 min
Condition 230/3.8; ASTM D1238
Plaskolite West Optix® CA-927 Impact Modified Acrylic Resin
Injection Molding Grade Pellets. Better impact strength than CA-924. Excellent surface gloss, optical clarity, and practical toughness.
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D-1238
Plaskolite West Optix® CP - 927 G High Impact Acrylic Resin
Optix® impact-modified grades exhibit 7 to 10 times the impact strength of general purpose grades and maintaining the superior optical properties. Each grade is offered in a grade(G) that resists g..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 200 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 392 °F
Procedure A; ASTM D1238
PolyOne Maxxam™ DC-818.G001-8000 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
RheTech Products GC30P103-01 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Black
Applications: Battery traysFender apronsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
Procedure A Condition G; ASTM D1238
Network Polymers NPP 808 C3WW
Description: Polycarbonate AlloyInformation provided by Network Polymers Inc.
Melt Flow 4.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
4.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific)
Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only.
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
Plaskolite West Optix® CA-927 G Clear Impact Modified Acrylic Resin
Impact modified acrylic resin, injection molding gradeApplications: An impact-modified acrylic resin designed for medical or food uses. This resin offers impact strengths up to seven times of gener..
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
Celanese Celanex® 1700FC PBT  (Unverified Data**)
Celanex 1700FC is a very high molecular weight extrusion grade of unreinforced polybutylene terephthalate for use in food contact applications.high molecular weight, unfilled PBT for use in food con..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Novapol® LE-0520-AM LDPE Extrusion Resin  (discontinued **)
Features: easy processing, good dispersion.Applications: extrusion coating.Data provided by the manufacturer.
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating  (discontinued **)
Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen..
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
Hyosung Topilene J440F PP
J440F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
I. Stern GPPS-004 General Purpose Crystal Polystyrene
Features:High Strength GradeMedium Flow, High ToughnessExcellent ProcessabilityApplicationsInjection MoldingAgency RatingsFDA Title 21 CFR 177.1640UL File E185934Information provided by I. Stern & C..
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
LyondellBasell Microthene® G MN72200 Low Density Polyethylene
General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop..
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
KKPC Kuhmo GP 150 High Heat Resistant, High Rigidity GPPS
Key features: High Heat-resistance, High Strength Common Uses: Vegetable boxes in refrigerators, humidifiers, lighting apparatus, cassette tape cases, parts of optical instruments, PS paper, etc.GPP..
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Iran Petrochemical (PCC) HIPS 7240 High Impact Polystyrene
HIPS7240 is a very high impact polystyrene used in the extrusion industry. The good melt strength of this grade makes it particularly suitable for deep-draw thermoforming. HIPS 7240 is available in ..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 343 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
Solvay Specialty Polymers Veradel® 3330GF Polyethersulfone (PESU), 30% Glass Fiber
Veradel® 3330GF is a 30% glass fiber reinforced grade of polyethersulfone (PESU). Adding glass fiber to polyethersulfone substantially increases the rigidity, tensile strength, creep resistance, ..
Melt Flow 4.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 60
Styron MAGNUMâ„¢ 3904 Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 3904 is a resin with super-high impact. It is used in a wide range of technical applications. It can be processed by injection molding, extrusion or thermoforming. The mass (c..
Melt Flow 4.5 g/10 min

@Load 3.80 kg,
Temperature 230 °C
4.5 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Techmer ES Plastiblend® ABS 92RK
Availability: North AmericaForms: PelletsFeatures: General PurposeProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 300 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS
Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl ..
Melt Flow 4.5 - 7.5 g/10 min

@Temperature 230 °C
4.5 - 7.5 g/10 min

@Temperature 446 °F
ASTM D1238
A. Schulman POLYFORT™ PP 3153 Homopolymer Polypropylene
DescriptionPolyfort® PP 3153 is a homopolymer polypropylene.Information provided by A. Schulman.
Melt Flow 4.5 g/10 min
4.5 g/10 min
ExxonMobil Method
ExxonMobil EXACT™ 4049 Plastomer for Elastic Film and Elastic Film Blends
Product Description: Exact 4049 is an ethylene-based butene plastomer produced using ExxonMobil Chemical’s EXXPOL® Catalyst Technology. This resin is designed for use as the cling component in mul..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Exceed™ 4518PA Metallocene Polyethylene Resin (European Grade)
Product Description: Exceed 4581PA is a metallocene ethylene-hexene copolymer. Films made of Exceed 4581PA have outstanding tensile properties and impact and puncture toughness. These superior prope..
Melt Flow 4.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
condition E; ASTM D1238
DuPont™ Surlyn® 9150 Ionomer Resin, Zinc
Surlyn® 9150 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The high MAA content and mi..
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Diamond Polymers NPP 808 C3 TDS Polycarbonate Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 4.5 g/10 min

@Load 21.6 kg,
Temperature 150 °C
4.5 g/10 min

@Load 47.6 lb,
Temperature 302 °F
ISO 1133
Fainplast Compounds Hax™ HFX 515 Crosslinkable HFFR Cable Compound
Polyolefin based HFFR silane grafted compound; cross-linkable by heat and moisture and by addition of suitable catalystGrade description:• Sheathing, InsulationInformation provided by Fainplast Com..
Melt Flow 4.5 g/10 min
4.5 g/10 min
ASTM D1238
M. Holland Company MAGMA® LM311-DX LLDPE  (discontinued **)
Features: Good Processability, Good Puncture Resistance, Good Tear Strength, Good ToughnessProcessing Method: ExtrusionInformation provided by M. Holland.
Melt Flow 4.5 - 7.5 g/10 min

@Load 1.05 kg,
Temperature 400 °C
4.5 - 7.5 g/10 min

@Load 2.31 lb,
Temperature 752 °F
ASTM D1238
Mitsui AURUM® PL450C Polyimide  (discontinued **)
AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU..
Melt Flow 4.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
4.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po..