Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 248 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Nye Lubricants 274L (SO) Synthetic Oil
Information provided by Nye Lubricants.
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Nye Lubricants 361F (RL) Synthetic Oil
Information provided by Nye Lubricants.
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Nye Lubricants 670 (NG) Synthetic Oil
Information provided by Nye Lubricants.
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Nye Lubricants 675(IF) Synthetic Oil
Information provided by Nye Lubricants.
Maximum Service Temperature, Air 120 °C
248 °F
Recommended
Nye Lubricants 774VH (NG) Synthetic Oil
Information provided by Nye Lubricants.
Maximum Service Temperature, Air 120 °C

@Time 1.80e+7 sec
248 °F

@Time 5000 hour
Continuous
Nylacast Nylube GF Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant), Glass Filled
For applications requiring higher compressive strength the NYLUBE GF masterbatch incorporates hollow glass ovule, designed to float and evenly distribute through the polymerising polymer. The glass ..
Maximum Service Temperature, Air 120 °C
248 °F
Precision Polymer Engineering N70F Nitrile Rubber
Nitrile Butadiene Rubber (NBR), 65-75 °IRHD. Copolymer of acrylonitrile and butadiene. Formulated using only those ingredients determined by the United States Federal Food and Drug Administration ..
Maximum Service Temperature, Air 120 °C
248 °F
Precision Polymer Engineering N90E Nitrile Rubber
High Nitrile Rubber, 85-95 °IRHD. High acrylonitrile (ACN) content. Copolymer of acrylonitrile and butadiene. ASTM designation = NBR. ISO designation = NBR. Aerospace Material Specification DTD5509..
Maximum Service Temperature, Air 120 °C
248 °F
Continuous; FRISETTA Test Method
Nilit FRIANYL A63 HH-KV15 Nylon 6.6 for injection molding, 15% glass ball reinforced
Nylon 6.6 for injection molding, heat and hydrolysis stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Maximum Service Temperature, Air 120 °C
248 °F
Continuous; FRISETTA Test Method
Nilit FRIANYL B63 TF30 Nylon 6 for injection molding, 30% PTFE lubricated
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
Maximum Service Temperature, Air 120 °C
248 °F
for short periods
Quadrant EPP Cestilene™ HD 500 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Maximum Service Temperature, Air 120 °C
248 °F
Resin Technology Group TIGA 202-EX High Performance, Fast Cure Adhesive
Mix ratio 2 to 1 by volume.TIGA 202-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 202-EX offers a 20 minute pot life and good hardness development within..
Maximum Service Temperature, Air 120 °C
248 °F
Resin Technology Group TIGA 216-EX High Performance Adhesive
Mix ratio 2 to 1 by volume.TIGA 216-EX is a two-part epoxy adhesive offering outstanding shear tensile and peel adhesion. TIGA 216-EX offers a 60 minute pot life and good hardness development within..
Maximum Service Temperature, Air 120 °C
248 °F
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System
Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas..
Maximum Service Temperature, Air 120 °C
248 °F
Lehmann & Voss LUVOCOM® 1850-7431 PBT, with carbon fiber and glass spheres
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Low waterabsorbtion, for dimensional stable precision parts.Par..
Maximum Service Temperature, Air 120 °C
248 °F
short term
Lehmann & Voss LUVOCOM® 3-8266 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
Maximum Service Temperature, Air 120 °C
248 °F
short term
Lehmann & Voss LUVOCOM® 80-0837 Polyacetal-copolymer, with PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Emergency running property, gl..
Maximum Service Temperature, Air 120 °C
248 °F
short term
Lehmann & Voss LUVOCOM® 80-7555/BK Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Maximum Service Temperature, Air 120 °C
248 °F
short term
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Maximum Service Temperature, Air 120 °C
248 °F
Maximum Operating Temperature
Industrial Laminates/Norplex ES-3 Engraving Stock
Description: Contains black phenolic/paper core and various colored covers impregnated with melamine resin.
Maximum Service Temperature, Air 120 °C
248 °F
LATI Latamid 12 G/50 PA 12, 50% Glass Fiber Reinforced
Polyamide 12 (PA12) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p.A.
Maximum Service Temperature, Air 120 °C
248 °F
Continuous
Schwartz Technical Plastics LAMINEX® 2010 Cotton Fabric, Phenolic Resin Impregnated, Fine
Application: slippers, inserts for coupling boxes, rollneck bearingsInformation provided by Schwartz Technical Plastics GmbH
Maximum Service Temperature, Air 120 °C
248 °F
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive
TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This ..
Maximum Service Temperature, Air 120 °C
248 °F
Trelleborg E715 EPDM Rubber
EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and ..
Maximum Service Temperature, Air 120 °C
248 °F
Trelleborg E935 EPDM Rubber
EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and ..
Maximum Service Temperature, Air 120 °C
248 °F
Dry
Chesterton MRS SD4i Metal Rebuilding System
An advanced ceramic composite for resurfacing and protection of metal surfaces in immersion service. It is normally applied in a thickness range of 250-370 microns (10 – 15 mils) per coat. Non-shri..
Maximum Service Temperature, Air 120 °C
248 °F
Elmer's Products Aron Alpha® 432TB Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
Maximum Service Temperature, Air 120 - 130 °C
248 - 266 °F
long term; EMS
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40
Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following ..
Maximum Service Temperature, Air 120 °C
248 °F
Elmer's Products Aron Alpha® 403T Cyanoacrylate Adhesive (Industrial Krazy Glue™)
Extra tough adhesives with highest heat, peeling, impact and thermal shock resistance.High gap fill. Ethyl base monomer. Excellent on rubber/plastic substrates. Excellent on metal substrates. Fa..
Maximum Service Temperature, Air 120 °C
248 °F
Abatron AboWeld 8505-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
AboWeld 8505-1 A/B is a solventless silver-epoxy adhesive and resurfacer. It has high rigidity, chemical and heat resistance. It also has good adhesion to most rigid materials.
Copyright © lookpolymers.com All Rights Reserved