Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Temperature = 232 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Melt Temperature 204 - 232 °C
400 - 450 °F
Polymer Resources PPX-FR2-[color]EN Modified PPO, UL 94 V-1 with HDT of 210 F, Extrusion Grade
Process: ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company RTP 700 A FR Low Density Polyethylene (LDPE), Flame Retardant
Melt Temperature 227 - 232 °C
441 - 450 °F
Chevron Phillips Vytek™ V208A Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Melt Temperature 227 - 232 °C
441 - 450 °F
Chevron Phillips Vytek™ V208E9 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart drop impact, hot-tack and heat seal properties, good drawdown, can b..
Melt Temperature 210 - 232 °C
410 - 450 °F
Stock
PolyOne Lubri-Tech™ SY-000/05T High Impact Styrene - 5% PTFE  (discontinued **)
Data provided by PolyOne.
Melt Temperature 193 - 232 °C
379 - 450 °F
Injection
Chevron Phillips K-Resin® BK12 Styrene-Butadiene Copolymer, Injection Molding Grade  (discontinued **)
Styrene-Butadiene CopolymerCustomer Benefits: BK12 is an SBC consisting of KR01 grade with a mold release added for easier processing. BK12 molded parts give excellent detail on fast production cyc..
Melt Temperature 199 - 232 °C
390 - 450 °F
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced
Information provided by FIBERFIL Engineered Plastics
Melt Temperature 199 - 232 °C
390 - 450 °F
Fiberfil® J-60/10/CC/30/E NATL Polypropylene Homopolymer, 10% FiberGlass and 30% Calcium Carbonate Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Melt Temperature 199 - 232 °C
390 - 450 °F
Fiberfil® J-60/30/E Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled
Information provided by FIBERFIL Engineered Plastics
Melt Temperature 210 - 232 °C
410 - 450 °F
Ineos Nova Zyntar® 7000 Flame Retardant Polystyrene
Features:General purpose workhorse resinGood flow for injection moldingUL94 V-0 @ 1.5 mm for all colors UL94 5VA rating FOAMED @ 4.6 mm, 0.87-1.07 g/cc density, natural colorCustom colors availableA..
Melt Temperature 193 - 232 °C
380 - 450 °F
LTL Color Compounds ColorFast® FRA204 ABS
High gloss, excellent impact ABS, V0/5VA-ratedAll information provided by LTL Color Compounders, Inc.
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company ESD C 100 MF Polypropylene (PP), ESD Protection - Electrically Conductive - Medium MFR
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 100 GB 10 Polypropylene (PP), Glass Bead
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 100 GB 20 Polypropylene (PP), Glass Bead
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 101 CC TFE 10 Polypropylene (PP), Glass Fiber - Chemically Coupled - PTFE Lubricated
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 103 CC HI HB Polypropylene (PP), High Impact - Glass Fiber - Chemically Coupled - UL94 HB
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 105 CC TFE 15 Polypropylene (PP), Glass Fiber - Chemically Coupled - PTFE Lubricated
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 154 HI Polypropylene (PP), Copolymer - Flame Retardant
The RTP 154 family of compounds are flame retarded, unreinforced polypropylene materials. They offer improved physical properties, low specific gravity and excellent moldability vs. traditional V-0..
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 183 TFE 15 Polypropylene (PP), Carbon Fiber - PTFE Lubricated
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 199 X 108940 B Polypropylene (PP), High Gravity Compound
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 199 X 132474 B Polypropylene (PP), Copolymer - Cellulose Fiber - 30% Renewable Resource Content
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 199 X 89849 B Polypropylene (PP), Glass Bubbles
Melt Temperature 182 - 232 °C
360 - 450 °F
RTP Company RTP 2720 S-50A Saturated Styrenic Block Copolymer
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP 199 X 134502 Polypropylene (PP) Glass Fiber - High Impact - Flame Retardant
Melt Temperature 193 - 232 °C
380 - 450 °F
Processing
ExxonMobil Santoprene® 201-64 Thermoplastic Elastomer
A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra..
Melt Temperature 149 - 232 °C
300 - 450 °F
Average value: 193 °C Grade Count:3
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min..
Melt Temperature 200 - 232 °C
392 - 450 °F
DuPont Elvax® 3200-2 Ethylene-Vinyl Acetate Copolymer Resin for Extrusion Coating
22.5 wt% Vinyl Acetate.Elvax® 3200-2 is an extrudable, wax-modified, ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process ..
Melt Temperature 185 - 232 °C
365 - 450 °F
Average value: 203 °C Grade Count:13
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..
Melt Temperature 193 - 232 °C
380 - 450 °F
RTP Company PermaStat® 400 Polystyrene (PS), ESD Protection - Permanently Anti-static
Melt Temperature 191 - 232 °C
375 - 450 °F
RTP Company RTP PP 30 GF FR0 BLK Polypropylene (PP), Glass Fiber - Flame Retardant - Value Product - UL94
Copyright © lookpolymers.com All Rights Reserved