Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products FT7012-707UV Thermoplastic Polyolefin, UV Stabilized, 848 Black Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products P250-01 Polypropylene Copolymer, Black Applications: ConsolesConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Petromont 4101 High Density Polyethylene Resin Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, f.. |
|||
Flexural Modulus | 1.17 GPa @Thickness 3.20 mm |
170 ksi @Thickness 0.126 in |
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A |
Pinnacle Polymers 2150 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products HP512-01 High Stiffness Polypropylene Copolymer, UV Stabilized, Black Applications: Automotive interior applicationsSeat back trimCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products HP513-538UV High Stiffness Polypropylene Copolymer, UV Stabilized, W12A 848 Black Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 13% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
M. Holland Company PP100 Polypropylene Homopolymer, General Purpose High clarityHomopolymerGood melt strengthHigh tensile strengthApplications: Thin-walled partsSheetStrapping |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
M. Holland Company RP700 Polypropylene Copolymer Features: Antistatic, Medium Clarity, Good FlowUses: Household Goods, KitchenwareApprovals: FDA 21 CFR 176.170(c), Table 2, Cond. B, C, D, E, F, G and HProcessing Method: Injection MoldingInformatio.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Global GPP-2500 Polypropylene Impact Copolymer, Nucleated Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 1.17 GPa @Temperature 23.0 °C |
170 ksi @Temperature 73.4 °F |
D790B |
Ineos T20N-00 Polypropylene Impact Copolymer This is a special high melt flow, nucleated, high impact copolymer polypropylene for injection molding applications. It offers excellent impact resistance and a high flexural modulus.ApplicationsCo.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PCC 0412 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1% Secant, 0.05 in/min; ASTM D790 |
LyondellBasell Pro-faxâ„¢ SD183 Polypropylene Copolymer Description: Pro-faxâ„¢ SD183 medium impact polypropylene copolymer resin is extremely resistant to aging at elevated temperatures in both wet and dry environments. It has an excellent balance of.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent, 0.05 in/min; ASTM D790 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene Impact Copolymer for Extrusion Applications Formolene® 2302E is a low flow, medium impact polypropylene copolymer designed for extrusion applications. It is a barefoot resin with a basic stabilizat.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
A. Schulman PP 2407 Polypropylene Impact Resistant Copolymer Polypropylene DescriptionPolypropylene PP 2407 is a low flow, impact resistant copolymer polypropylene. Information provided by A. Schulman. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1.3mm per min, 1% secant; ASTM D790 |
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions.Formolene 6502A is a medium impact copolymer with an excellent balance of t.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | DIN EN ISO 178 |
Wolf Kunststoff ZEDEX® ZX-550 A5L Polymer Alloy Main Characteristics: Strong anti-adhesive; Low creep; Weather resistant; No water absorption; Good machinability; Strongly viscoelastic; Stress resistantApplications: Chemical Engineering; Laborato.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Total PPR 3230XZ Polypropylene, Blow Molding Grade Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ BA50-120 High Density Polyethylene Resin Product Description: BA50-120 is a high molecular weight, high density polyethylene copolymer. This resin has superior stress crack resistance, high impact strength and good rigidity.Availability: .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Clariant Renol PA2SP0003 Nylon 6, High Gloss Data provided by Clariant Masterbatches |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Dow UNIPOL™ DGDA-5110 Polyolefin DGDA-5110 UNIPOL™ is designed for the manufacture of thermoformed truck liners and other sheet extrusion applications requiring toughness and good process-ability. Information provided by Dow |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Secant @ 1% strain; ASTM D790 |
Bapolene® PP5083 Polypropylene, Injection Grade Bapolene PP 5083 is a clarified PP Random Copolymer for injection molding. This resin exhibits good processing and impact properties. This product meets FDA regulation 21CFR 177.1520 and is suitab.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B900 (Base Grade), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9086 (FDA Odor Mask), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | SAE J949 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1.3 mm/min, 1% Secant; ASTM D790 |
Amco PRIMATOP PP CO 120-11 RC Random Copolymer Features:medium flowcontains clarifying agentexcellent clarityApplications:storage boxesvialscontainersFormer A-Top Polymers product; part of Amco product line since 2013. |