Material Notes:
General Purpose Unreinforced; High Flow. Property data for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0090 - 0.016 cm/cm
0.0090 - 0.016 in/in
Linear Mold Shrinkage, Transverse 0.010 - 0.017 cm/cm
0.010 - 0.017 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 52.0 MPa
7540 psi
ASTM D638
Flexural Yield Strength 83.0 MPa
12000 psi
ASTM D790
Flexural Modulus 2.30 GPa
334 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 227 °C
441 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 154 °C
309 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.0 °C
129 °F
ASTM D648