Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products FT4700-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent; ASTM D790 |
RheTech Products P251-01 Polypropylene Copolymer, Black Applications: Splash shieldFuse panel coversCenter consolesDoor panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 30-0500 A Description: Homopolymer Polypropylene with AntistaticInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Petromont 4101 High Density Polyethylene Resin Petromont HDPE 4101 is a high density polyethylene copolymer resin produced using the UNIPOL® Process. This resin is primarily used in the extrusion of corrugated pipes for drainage applications, f.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers SEQUEL® 1440LS TPO
(discontinued **) Description: SEQUEL® 1440LS engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, excellent processabilit.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
NOVA Chemicals Sclair® 58D HDPE Blow Molding Resin
(discontinued **) Features: Good ESCR, high stiffness, good impact strength, slightly tougher alternative to Sclair 58A.Applications: Small part blow molding, food, pharmaceuticals, HIC containers.Data provided by th.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CH085S Polypropylene, Homopolymer, Cast Film, Slip COPYLENE™ CH085S is a controlled rheology polypropylene homopolymer resin containing slip additive. COPYLENE™ CH085S is used in injection molding and cast film extrusion applications. Applications.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B902 (UV Inhibitor Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9024 (UVI, Odor Mask Added), 10% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP801 (UV Inhibitor Added), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
M. Holland Company CP402 Polypropylene Impact Copolymer Impact copolymerGood impact resistanceLow temperature impact resistanceNucleatedGood stiffnessApplications: CratesLawn and garden equipmentTool/tote box |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PCC 0412 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Tangent, 0.05 in/min; ASTM D790 |
LyondellBasell Hostacomâ„¢ RTA3184 Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RTA3184 medium melt flow, 1,300 MPa flexural modulus, low level glass-reinforced, colorable, interior trim grade thermoplastic elastomeric olefin (TEO) resin is modified .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Total PPR 3230XZ Polypropylene, Blow Molding Grade Homopolymer Blow Molding GradeLubricated – FINA 3230XZ offers superior core road release, eliminating the need for additional lubricant.Antistat – FINA 3230XZ contains antistat to minimize dust ac.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D 790 |
Total PPC 4824WZ Polypropylene, Impact Copolymer ATOFINA 4824WZ is a nucleated impact copolymer. 4824WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. It has been formulated for excellent .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | |
CMW® ELKONITE® 30W3 Infiltrated Copper Tungsten contact material ASTM B702, Class E, infiltrated, RWMA Class 12 For projection welding dies, die facing, and resistance welding electrodes. Also used for low expansion structural members. Information provided by CMW Inc. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem CP360H Homopolymer Polypropylene Description: Narrow MWD, Low Smoke / CondensateApplications: Suggested Uses Include Fine Denier Spunbond Nonwovens, High-Speed Spinning - Continuous Filament YarnThis resin meets the requirements fo.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | Secant @ 1% strain; ASTM D790 |
Bapolene® PP5083 Polypropylene, Injection Grade Bapolene PP 5083 is a clarified PP Random Copolymer for injection molding. This resin exhibits good processing and impact properties. This product meets FDA regulation 21CFR 177.1520 and is suitab.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Arkema Group Solarkote® P-600 Acrylic PVC Capstock, clear, high glossInformation provided by Arkema Group |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 12% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and .. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | SAE J949 |
Azdel SuperLite® SL551400-100 PP Resin Matrix / 55% Glass Fiber (4 mm Molded Thickness) AZDEL SuperLite® SL551400-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Formosa Plastics Formolene® HL5010 Blow Molding HDPE Extra High Molecular Weight Hexene CopolymerApplications: Blow Molded 55-gallon shipping containers, gasoline tanks, agricultural chemical tanks; Extruded pallets, cattle feeders, large formed parts.. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790 |
Chase Plastics CP Pryme® PPC100-35M Polypropylene Copolymer Information provided by Chase Plastics. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | ASTM D790A |
BP Amoco Acctuf® 3638 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Compounding, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Flexural Modulus | 1.17 GPa | 170 ksi | 0.05 in/min, 1% secant; ASTM D-790A |
Braskem TI6120AN High Impact Copolymer Polypropylene Description: Excellent balance of toughness and stiffness, unique dimensional stability and excellent flow properties.Applications: Suggested uses include compounding, injection molding, automotive .. |