Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.320 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.599 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ JN-818.S001-1000 Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.599 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Nymax™ GB 1200 20 HS BLACK 18 Polyamide 66 (Nylon 66) Preliminary Data SheetMolded Test Bars: Dry as MoldedInformation provided by PolyOne |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC PP 506P Polypropylene Homopolymer for Raffia Applications Product Description: PP 506P is intended for producing low denier stretched tapes with the following features:Consistent processabilityGood processability at high line speeds and low deniersLow tap.. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.599 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ 34-1520 Silver Metallic TFPP Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.320 J/cm @Thickness 3.18 mm, Temperature 23.0 °C |
0.599 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
Injection Molded; ASTM D256A |
PolyOne Maxxam™ 34-1520 SSM TFPP Polypropylene Homopolymer (PP Homopolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Izod Impact, Notched | 0.320 - 2.94 J/cm | 0.599 - 5.51 ft-lb/in | Average value: 1.05 J/cm Grade Count:35 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Izod Impact, Notched | 0.320 - 0.801 J/cm | 0.599 - 1.50 ft-lb/in | Average value: 0.575 J/cm Grade Count:26 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Izod Impact, Notched | 0.320 - 2.00 J/cm | 0.599 - 3.75 ft-lb/in | Average value: 0.595 J/cm Grade Count:41 |
Overview of materials for Polyetherimide (PEI), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
LNP ULTEM® EXCP0096 Polyetherimide, 30% Carbon Fiber Reinforcement, 10% PTFE Lubricant
(discontinued **) Features: Lubricated, Electrically Conductive, Good Wear Resistance, High Heat ResistanceForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This dat.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Conditioned) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP STAT-KON KEP33 Acetal LNP STAT-KON* KEP33 is a compound based on Acetal resin containing 15% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific) LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific) LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RB008 PA 66 (Asia Pacific) LNP THERMOCOMP* RB008 is a compound based on Nylon 66 resin containing Glass Bead. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RW004 PA 66 (Asia Pacific) LNP* THERMOCOMP* RW004 is a compound based on Nylon 66 resin containing Mineral. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RZ0069 PA 66 (Asia Pacific) LNP* Thermocomp* RZ0069 is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant, Milled Glass. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RZ006S PA 66 (Asia Pacific) LNP* Thermocomp* RZ006S is a compound based on Nylon 66 resin containing Milled Glass. |
|||
Izod Impact, Notched | 0.320 J/cm @Temperature 23.0 °C |
0.599 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP WH0450EX PBT (Asia Pacific) LNP* Thermocomp* WH0450EX is a compound based on Polybutylene Terephalate resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RW004 PA 66 LNP THERMOCOMP* RW004 is a compound based on Nylon 66 resin containing Wollastonite. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman PP 3466-01 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3466-01 is a homopolymer polypropylene with the addition of antistatic. This product enhances processing with fast cycle times in injection molding.ApplicationPP 3466-01.. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ FPP 1006S Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1006S is a 20% talc filled homopolymer polypropylene compound formulated with an internal mold release. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ FPP 1007E Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007E is a 40% talc filled homopolymer compound for extrusion applications.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFORT™ FPP 1237 CaCO3 filled homopolymer polypropylene DescriptionPolyfort® FPP 1237 is a 20% CAC03 filled homopolymer polypropylene product. Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman POLYFLAM™ FPP 1007 Talc Filled Homopolymer Polypropylene DescriptionPolyfort® FPP 1007 is a 40% talc filled homopolymer polypropylene compound.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
Chang Chun Plastic Longlite PM T310 Impact Phenolic Molding Compound ASTM Grade per ASTM D700 is 13.Information provided by Dowell Trading Company Ltd. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 272 Polystyrene Alloy, Glass Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Notched | 0.320 J/cm | 0.599 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 628 Nylon 6/6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |