Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON WSF42 PBT (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP*STAT-KON* WSF42 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Stainless Steel Fiber. Added features include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 73.0 MPa
10600 psi
5 mm/min; ISO 527
Elongation at Break 2.3 %
2.3 %
5 mm/min; ISO 527
Tensile Modulus 6.40 GPa
928 ksi
1 mm/min; ISO 527
Flexural Yield Strength 112 MPa
16200 psi
2 mm/min; ISO 178
Flexural Modulus 6.30 GPa
914 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²
2.38 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 43.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
23.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
CTE, linear, Transverse to Flow 118 µm/m-°C

@Temperature 23.0 - 60.0 °C
65.6 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
Electrical Properties Metric English Comments
Surface Resistance 100 ohm - 1e+05
100 ohm - 1e+05
ASTM D257