Techmer ES Electrablend® POM Acetal

Category Polymer , Thermoplastic , Acetal (POM)
Manufacturer Techmer ES
Trade Name Electrablend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® POM Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Melt Flow 2.0 g/10 min

@Load 10.0 kg,
Temperature 230 °C
2.0 g/10 min

@Load 22.0 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 56.5 MPa
8200 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Flexural Modulus 3.03 GPa
440 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm

@Thickness 3.17 mm
0.600 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 107 °C
225 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 50 ohm-cm
50 ohm-cm
ASTM D257
Surface Resistance 50 ohm
50 ohm
ASTM D257