Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.03 GPa | 440 ksi | Tangent; ASTM D790 |
RheTech Products FRP257-00 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Natural Applications: Electrical component housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | ASTM D790 |
PolyOne Maxxam™ PPC-20G Nat Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | ASTM D790 |
PolyOne Geon™ Vinyl Fittings M1012 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago |
|||
Flexural Modulus | 3.03 - 14.8 GPa | 440 - 2150 ksi | Average value: 7.75 GPa Grade Count:104 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PEI1000 Polyetherimide Injection and extrusion grade polyetherimide, high temperatureAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® PSU1700 Polysulfone General purpose polysulfone with excellent clarityAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | |
Ineos Styrenics Polystyrene 145D (NAFTA) A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics pu.. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem HTX1010F PEI (Asia Pacific) Higher impact, Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES Electrablend® POM Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® POM CO 0167 S1 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® POM HO 0167 S1 Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: HomopolymerInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 439 ksi | 2.6 mm/min, 100 mm span; ASTM D 790 |
SABIC Innovative Plastics Noryl PKN4717 PPE+PS (Asia Pacific) PPE+PS. Translucent. FDA compliant. High heat. Foam extrusion. Microwavable. Food packaging uses. Solid properties listed.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® PBT 0158 S Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Techmer ES HiFill® PPSU A1 0200 B LE Availability: North AmericaForms: PelletsFeatures: High Density and Low ExtractablesAppearance: OpaqueInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Ensinger Tecatron® XP-76 Compression Molded PPS Compound, 55% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D-790 |
Axiall 6316 Rigid PVC, Molding Georgia Gulf 6316 is an economical high flow rigid PVC fittings compound designed for drain, waste and vent applications, where higher impact properties are desired. This compound is characterized .. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D-790 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | ASTM D790 |
Asahi Kasei Thermylene® P6-20FM-2601 20% Glass/Mineral, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | 2.0 in/min; ASTM D790 |
LTL Color Compounds ColorFast® NY2 Nylon 66 Nylon 6,6 with or without lubeAll information provided by LTL Color Compounders, Inc. |
|||
Flexural Modulus | 3.03 GPa | 440 ksi | secant; ASTM D790 |
Spartech PP5340 Mica Reinforced Homopolymer Information provided by Spartech |