Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Oxford Polymers C-Acetal 10MF-900 BK Acetal Product Description: Acetal Injection Molding Grade, 10 melt flow Processing and Delivery Form: Pellets and Injection MoldingSpecial Characteristics: Pre-colored blackInformation provided by Oxford.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C @Thickness 3.20 mm |
225 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C @Thickness 3.20 mm |
225 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C @Thickness 3.20 mm |
225 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C @Thickness 3.20 mm |
225 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C @Thickness 3.20 mm |
225 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C @Thickness 3.20 mm |
225 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
Polymer Resources PPX-GP3-[color]-HF Modified-PPO, General Purpose, High Flow Modified-Polyphenylene Oxide, General Purpose, High Flow, 235F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test sample.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
Polymer Resources PPX-GP3 Modified PPO, General Purpose with HDT of 235 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
Quadrant EPP Semitron® ESd 225 POM-C, static dissipative, extruded (ISO Data) Semitron ESd 225 is an acetal based static dissipative material ideal for material handling operations. It is also an excellent choice for fixturing used in the manufacturing of hard disk drives or .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C @Thickness 6.40 mm |
225 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Xenoy® 1731 PBT+PC (Asia Pacific) Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | |
Saint-Gobain Rulon® 125 Bearing/Seal PTFE Rulon 125 is used primarily in applications that are not severe such as dryer drum slides and piston rings in pneumatic or hydraulic controls.Information provided by distributor TriStar Plastics Cor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Techmer ES Plastiblend® PC/ABS 1110 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | unannealed; ASTM D648 |
Styron Pulse® 2100LG ABS + PC Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL NH4030B PPE+HIPS (Asia Pacific) NH4030B is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nory.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics NORYL EXNL0303 PPE+HIPS (Europe-Africa-Middle East) EXNL0303 is a modified PPE-HIPS blend that presents an excellent balance of non halogenated flame retardance, lower smoke production upon burning and low specific gravity for light weight parts. Nor.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
Ecomass® 1080ZD96 Tungsten Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityTungsten Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided b.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
Ecomass® 1080ZG90 Metal Filled Polyamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applications.High Specific GravityMetal Powder Filled Polyamide (PA) AlloyExcellent ToughnessInformation provided by T.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Delrin 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage less s.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ISO 75-1/-2 |
DuPont Performance Polymers Delrin® 511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 - 149 °C | 225 - 300 °F | Average value: 132 °C Grade Count:6 |
Overview of materials for Polycarbonate, Glass Fiber & Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber & Bead Filled". Each property range of values reported is minimum and maximum.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | ASTM D648 |
Chase Plastics CP Pryme® PCA100 Polycarbonate/ABS Alloy Information provided by Chase Plastics. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 107 °C | 225 °F | |
Arkema Group Kynar® 4000 HD PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b.. |