Mechanical Properties Metric English Comments
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
PolyOne Maxxam™ PPR-20G Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
PolyOne Maxxam™ PPR-20G Nat Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
PolyOne Trilliant™ HC HC5210-0020 RS Natural Polypropylene Homopolymer (PP Homopolymer)
Information provided by PolyOne
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Network Polymers Kepital® F20-03
Description: Natural Acetal CopolymerInformation provided by Network Polymers Inc.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP2-[color]-3 Acetal Copolymer, Medium Flow, General Purpose Molding, UV Stabilized
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP2-UV Acetal Copolymer, Medium Flow, UV-stabilized
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
PolyOne Geon™ Vinyl Dry Blend E7456 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Wall Applications
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation.
Flexural Strength 90.3 MPa

@Temperature 130 °C
13100 psi

@Temperature 266 °F
ASTM D-790
Glastic 1120 Corrosion-Resistant Panels
Glastic® Corrosion-Resistant Panels are ideal for applications where resistance to both flame, and the splash or spill of laboratory chemicals is important. Glastic® Grade 1120 is an asbestos..
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Techmer ES Electrablend® POM Acetal
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Saint-Gobain Meldin® 7022 Isostatically Molded Graphite Filled Polyimide
Finished parts and basic shapes made from 40% by weight graphite filled polyimide material for applications requiring a low coefficient of thermal expansion, self lubricating properties, and good di..
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Chase Plastics CP Pryme® AC100-27 Acetal Copolymer Molding Resin
Information provided by Chase Plastics.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Chase Plastics CP Pryme® AC100-9 Acetal Copolymer Molding Resin
Information provided by Chase Plastics.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength  (Unverified Data**)
Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP2 Acetal Copolymer, Medium Flow, General Purpose Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Strength 90.3 MPa
13100 psi
ASTM D790
Polymer Resources AC-GP3 Acetal Copolymer, High Flow, Thin Walled Molding  (Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.