Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Polymer Resources NY6/12-GP1 General Purpose Nylon 612 Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide.. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Polymer Resources PC-G10-IM Polycarbonate, 10% Glass Reinforced, Impact Modified Polycarbonate, 10% Glass Reinforced, Impact ModifiedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information .. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Polymer Resources PPX-FR1-[color]-EN Modified-PPO, V-0 Flame Retardant, Extrusion Grade Modified-Polyphenylene Oxide, V-0 Flame Retardant, 190F HDT, Extrusion GradeFeatures: • Bromine Free • Chlorine FreeProcess: ExtrusionNotes: All physical, mechanical and thermal testing conducte.. |
|||
Tensile Strength, Yield | 56.5 MPa | 8190 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® XT XT-100-BW00 Natural Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | |
Lord Adhesives Thermosetâ„¢ MD-130 Electrically Insulating Die-Attach Adhesive Lord MD-130 is a microelectronic grade, die-attach adhesive system for use in applications where electrical conductivity is not required. This system offers long, room temperature stability, fast cu.. |
|||
Tensile Strength, Yield | 56.5 MPa @Thickness 3.17 mm, Temperature 22.8 °C |
8200 psi @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D638 |
MRC Polymers NAXELLâ„¢ PC23MS Polycarbonate, Impact Modified, High MFR, EZ Flow Economy GradeImpact modifiedCan be UV stabilizedGenerally for black onlyInternal and external lubricant can be addedInformation provided by MRC Polymers Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Electrablend® POM Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES HiFill FR® ABS GF10 FR 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Flame RetardantUL File Number: E157318Information provided by TP Composites, I.. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES HiFill FR® ABS GF15 FR-2 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 1110 Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 2022 Availability: North AmericaForms: PelletsFeatures: Low GlossInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS 8001A Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS FR 1950 BK Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS FR 2810 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS FR 6206 Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES Plastiblend® PC/ABS FR 6206 UV Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES HiFill® PA6 0325 Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityTPC# 6066102Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | |
Tra-Con Tra-Cast 3107 Low Shrinkage Epoxy Casting System TRA-CAST 3107 is a versatile epoxy casting system developed for high performance production potting, encapsulating, casting and tooling applications where low shrinkage, easy handling and flowabilit.. |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Clariant Renol PA2SP0008HW Nylon 6, Heavyweight Compound Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 56.5 MPa | 8200 psi | ASTM D638 |
Techmer ES HiFill® TPU GF30 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc. |