Polymer Property : Surface Resistance = 50 ohm Product List

Electrical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties Metric English Comments
Surface Resistance 50 ohm
50 ohm
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced
Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Surface Resistance 50 ohm
50 ohm
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Surface Resistance 50 ohm
50 ohm
LATI Latiohm 82-02 PD09 PA12
Semiconductive/dissipative product based on Polyamide 12 (PA12). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industr..
Surface Resistance 50 ohm
50 ohm
LATI Latishield 36/AR-08A G/17-V0E ABS, Steel/Glass Fiber Reinforced, Flame Retardant
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Availability: Africa..
Surface Resistance 50 ohm
50 ohm
LATI Latishield 36/SP-05A ABS, Steel Fiber Reinforced
EMI shielding product based on Acrylonitrile-Butadiene-Styrene copolymer (ABS). Steel fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provid..
Surface Resistance 50 ohm
50 ohm
LATI Latishield 66-08A G/25-V0KB1 PA66, Steel/Glass Fiber Reinforced, Flame Retardant
EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Glass fibers. UL94 V-0 classified, with red phosphorous. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No..
Surface Resistance 50 ohm
50 ohm
LATI Latistat 52/7-02 PP Homopolymer
Dissipative product based on Polypropylene homopolymer (PPh). Unfilled. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T..
Surface Resistance 50 ohm
50 ohm
ASTM D257
Techmer ES Electrablend® POM Acetal
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Features: ConductiveTPCI# 9961114Information provided by TP Composites, Inc.
Surface Resistance 50 ohm
50 ohm
ASTM D257
Techmer ES Electrafil® J-1200/CF/30 ABS, 30% Carbon Fiber Reinforced
Surface Resistance 50 ohm
50 ohm
IEC 60093
EMS-Grivory Grivory® GCL-3H anthracite PA*-CF30
Product description: Grivory GCL-3H anthracite is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is reinforced by 30% long ca..
Surface Resistance 50 ohm
50 ohm
IEC 60093
EMS-Grivory Grivory® LC-3H black PA12-CF30
Product description: Grilamid LC-3H BLACK is a Polyamide 12 injection molding product reinforced with 30 % carbon fibers. The product is inherently black and is only available in this color.Main Att..
Surface Resistance 50 ohm
50 ohm
IEC 60093
EMS-Grivory Grivory® LCL-3 H anthracite PA12-CF30
Product description: Grilamid LCL-3H anthracite is based on a heat stabilized PA12 and 30% long carbon fibers. Grilamid LCL-3H anthracite is characterized by the following key-properties: high stiff..
Surface Resistance 50 ohm
50 ohm
IEC 60093
EMS-Grivory Grivory® LC-15H black PA12-CF15
Product description: Grilamid LC-15H black is a Polyamide 12 injection molding product reinforced with 15% carbon fibers. The product is inherently black and is only available in this color.Main Att..