| Category | Polymer , Thermoplastic , ASA Polymer |
| Manufacturer | Styrolution |
| Trade Name | Luran® |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Styrolution Luran® S 778 TE Black 25991 ASA.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
| Water Absorption | 1.65 % | 1.65 % | Equilibrium; ISO 62 |
| 0.45 % @Time 86400 sec |
0.45 % @Time 24.0 hour |
ISO 62 | |
| Moisture Absorption at Equilibrium | 0.35 % | 0.35 % | 23°C/50% RH; ISO 62 |
| Melt Flow | 5.35 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.35 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Ball Indentation Hardness | 85.0 MPa @Load 36.5 kg, Time 30.0 sec |
12300 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
| Tensile Strength, Yield | 54.0 MPa | 7830 psi | 50 mm/min; ISO 527-1/-2 |
| Elongation at Break | 8.0 % | 8.0 % | Nominal, 50 mm/min; ISO 527-1/-2 |
| Elongation at Yield | 3.4 % | 3.4 % | 50 mm/min; ISO 527-1/-2 |
| Tensile Modulus | 2.50 GPa | 363 ksi | ISO 527-1/-2 |
| Flexural Strength | 80.0 MPa | 11600 psi | ISO 178 |
| Charpy Impact Unnotched | 9.00 J/cm² @Temperature -30.0 °C |
42.8 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
| 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU | |
| Charpy Impact, Notched | 0.400 J/cm² @Temperature -30.0 °C |
1.90 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
| 1.50 J/cm² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA | |
| Tensile Creep Modulus, 1000 hours | 1250 MPa @Strain <=0.500 % |
181000 psi @Strain <=0.500 % |
ISO 899-1 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 80.0 - 110 µm/m-°C @Temperature 23.0 - 80.0 °C |
44.4 - 61.1 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/-2 |
| Thermal Conductivity | 0.170 W/m-K | 1.18 BTU-in/hr-ft²-°F | DIN 52612-1 |
| Maximum Service Temperature, Air | 90.0 °C | 194 °F | |
| Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ISO 75-1/-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 103 °C | 217 °F | ISO 75-1/-2 |
| Vicat Softening Point | 104 °C | 219 °F | VST/B/50; ISO 306 |
| 113 °C | 235 °F | VST/A/50; ISO 306 | |
| Flammability, UL94 | HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
IEC 60695-11-10 |
| HB @Diameter 4.00 mm |
HB @Diameter 0.157 in |
IEC 60707 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+12 ohm-cm | 1.00e+12 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Dielectric Constant | 3.5 @Frequency 1.00e+6 Hz |
3.5 @Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.9 @Frequency 100 Hz |
3.9 @Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 35.0 kV/mm | 889 kV/in | K20/P20; IEC 60243-1 |
| Dissipation Factor | 0.0090 @Frequency 100 Hz |
0.0090 @Frequency 100 Hz |
IEC 60250 |
| 0.033 @Frequency 1.00e+6 Hz |
0.033 @Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 600 V | 600 V | Test Liquid A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 200 - 240 °C | 392 - 464 °F | Extrusion, Pipes |
| 210 - 250 °C | 410 - 482 °F | Extrusion, Plates | |
| Drying Temperature | 80.0 °C | 176 °F | Pre-drying |
| Dry Time | 2 - 4 hour | 2 - 4 hour | Pre-drying |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Black 25991 | |
| Commercial Status | Europe | |
| Primary Processing Technique | Extrusion |