Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
SABIC PP 511A Polypropylene Homopolymer for Spunbond Applications Product Description: PP 511A is a controlled rheology grade with a narrow molecular weight distribution intended for spun bond fiber extrusion applications.PP 511A has the following features:Consis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Unannealed (0.250 in); ASTM D648 |
Ravago Manufacturing Americas Hysun™ 678 ASA Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families. Availibility: North America F.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 222 °F | Unannealed; ASTM D648 |
Ravago Manufacturing Americas Hysun™ A6020 ASA+PC Available in North America Features: Good Impact Resistance and High Heat Resistance RoHS CompliantForm: PelletsInformation provided by Ravago |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Unannealed; ASTM D648 |
PolyOne Edgetek® AS-10GF/000 FR V0 BLACK Acrylonitrile Butadiene Styrene (ABS) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Annealed, 80°C, 4 hours; ISO 75 |
LG Chemical LG-703A ABS, Low Gloss, General Purpose Information Provided by LG Chem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Unannealed; ASTM D648 |
Global PP-2540-K Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-paint drum, storage & transport containerInformation provided by Global Polymers Corporation. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
LG Chemical SEETEC H7525 Polypropylene, Homopolymer Features: Seetec H7525 is designed for the extrusion of staple fibers. This grade is characterized by Medium MWD and good thermobonding, with anti-gas fading stabilization. SEETEC H7525 meets the FD.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
LG Chemical SEETEC H7600 Polypropylene, Homopolymer Features: Seetec H7600 is designed for the extrusion of continuous filament (CF) and staple fibers. This grade is characterized by medium MWD and good heat stability. SEETEC H7600 meets the FDA requ.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
IRPC Polimaxx Polene 2541TC Polypropylene Block Copolymer CHARACTERISTICS: EXCELLENT FLOWABILITY, HIGH STIFFNESS, HEAT STABILITY, HIGH IMPACTAPPLICATIONS: INJECTION MOLDING SPECIALLY FOR WASHING TUB, ELECTRICAL APPLIANCES, THIN WALL CONTAINERS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ISO 75B |
Lucite International Diakon® MH254 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C @Thickness 3.20 mm |
223 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP STAT-KON AX02747 ABS LNP* STAT-KON* AX02747 is a compound based on ABS resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Unannealed; ASTM D648 |
Techmer ES HiFill FR® ASA FR-2A WT209 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant, Good Toughness and Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ASA 778 UV WT168 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C @Thickness 6.40 mm |
223 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xenoy® 1101 PBT+PC (Asia Pacific) Unreinforced, opaque polycarbonate/polyester alloy. Excellent low temperature impact plus chemical resistance to automotive fluid.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ISO 75-1/-2 |
Styrolution Luran® S 778 Q42 Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | annealed; ASTM Test |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ISO 75 |
Styrolution Luran® S 778 T ASA Luran S 778 T is an injection molding ASA grade with enhanced toughness and heat resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ISO 75-1/-2 |
Styrolution Luran® S 778 TE Black 25991 ASA Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ISO 75 |
Styrolution Novodur® 5300 ABS Novodur 5300 is a high heat injection molding grade with high impact strength, good chemical resistance and reduced emission (PC modified)Information provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | Annealed; ASTM D648 |
Techmer ES Plastiblend® ABS HH BK MB Availability: North AmericaForms: PelletsFeatures: High Gloss and High Heat ResistanceAppearance: BlackProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
Formosa Plastics Formolene® 6145O Impact Copolymer Polypropylene Impact Copolymer for Appliance Applications Formolene® 6145O is a medium impact copolymer of polypropylene characterized by its easy mold flow, physical property balance and excellent dimensional s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | 120°C per hour; ISO 752 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | 0.25 inch; ASTM D648 |
PlastxWorld CEVIAN® B14E0 PBT/ABS Alloy Excellent flowability, high impact strength and toughness. These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 222 °F | unannealed; ASTM D-648 |
Axiall ProTherm® 4351 Rigid PVC, Extrusion Georgia Gulf ProTherm® 4351 is a CPVC powder blend designed for extrusion of large diameter, heavy wall industrial grade pipe requiring high heat deflection temperatures and excellent chemical resi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
Braskem H 605 Thermoforming Polypropylene Applications: Flat and corrugated sheets with high transparency; thermoformed packing with high transparency. Information provided by Braskem |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0336M10L Mica Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
Cheng Yu Plastic A706G1 SAN, 10% Glass Fiber |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 106 °C | 223 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 213 Polystyrene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |