SABIC Innovative Plastics LNP THERMOTUF PF008IR PA 6 (Asia Pacific)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP Thermotuf
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP THERMOTUF PF008IR PA 6 (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Thermotuf* PF008IR is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact, Mold Release.
Physical Properties Metric English Comments
Density 1.46 g/cc
0.0527 lb/in³
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 143 MPa
20700 psi
ASTM D638
Elongation at Break 2.4 %
2.4 %
ASTM D638
Tensile Modulus 13.1 GPa
1900 ksi
50 mm/min; ASTM D638
Flexural Strength 255 MPa
37000 psi
ASTM D790
Flexural Modulus 9.85 GPa
1430 ksi
ASTM D790
Izod Impact, Notched 1.44 J/cm
2.70 ft-lb/in
ASTM D256
Izod Impact, Unnotched 11.21 J/cm
21.00 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 205 °C

@Thickness 3.20 mm
401 °F

@Thickness 0.126 in
unannealed; ASTM D648