Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite Optix® CA - 75 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 113 °C @Load 1.00 kg |
235 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Cycoloy® C1000 PC+ABS (Europe-Africa-Middle East) CYCOLOY C1000 is a PC+ABS blend developed with emphasis on excellent processing efficiency while maintaining good heat resistance and impact ductility. It is an excellent material choice for a wide .. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Europe-Africa-Middle East) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of propertiesThis data was supplied by.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX2244ME PC+ABS Cycoloy* CX2244ME resin is a flame retardant PC/ABS blend featuring excellent balance of flow and impact together with UL-94 V0 rating at < 1mm. Cycoloy CX2244ME resin also demonstrates improved che.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.2mm and 5VB at 1... |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240 resin is an injection moldable PC/ABS blend. It contains non-brominated and non-chlorinated flame retardant systems to meet UL-94 V0 at 0.75mm, V1 at 0.6mm, V2 at 0.4mm and 5VB at 1... |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Asia Pacific) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/120; ISO 306 |
SABIC Innovative Plastics Cycoloy® CX7240U PC+ABS (Europe-Africa-Middle East) Cycoloy* CX7240U resin is an injection moldable PC/ABS blend with a UV stabilization package. It contains non-brominated and non-chlorinated flame retardant systems to meet thin wall flame resistanc.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® ML7686 PC (Europe-Africa-Middle East) Transparent Polycarbonate in limited colors. Excellent processability, super high flow. UL rated V-2 at 1.5mm. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 75 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite West Optix® CP - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ISO 306 |
SABIC Innovative Plastics Lexan® DMX6014 PC Copolymer (Asia Pacific) DMX6014 is an injection moldable PC copolymer ABS blend. This resin combines excellent scratch resistance (F-pencil hardness) with ductility.This data was supplied by SABIC-IP for the Asia Pacific r.. |
|||
Vicat Softening Point | 113 °C | 235 °F | 50°C/hr; 50N |
Polimeri Europa SINKRAL B260 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,115-04-09-25 Very high heat injection moulding grade with good impact resistance for this category of ABS. Main.. |
|||
Vicat Softening Point | 113 °C | 235 °F | 1 kg; ASTM D1525 |
LG Chemical IH830H PMMA, General Purpose Grade for Injection Molding Highest of all grades in heat resistanceMechanical strength and surface hardnessParticularly recommended for tail lamp, reflectors, and general lighting fixturesFeatures: Excellent transparency and .. |
|||
Vicat Softening Point | 113 °C | 235 °F | ISO 306A |
Lucite International Diakon® MG100 Acrylic Bead Polymer, High Transparency PMMA beads offer an exceptional transmission level of 92.5%, an increase of +0.5% in light transmission vs. granular grades - ideal for medical diagnostic devices.Information provided by Lucite Inte.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D1525 |
LyondellBasell DP 0110M Polybutene Key Features: highly isotactic, semi-crystalline nucleated homopolymer, good creep resistance, good environmental stress crack resistance, FDA acceptable, easily dispersibleApplications: packaging i.. |
|||
Vicat Softening Point | 113 °C | 235 °F | B/50; ISO R306 |
Samsung Cheil Industries Starex® SR-0325LTS ABS, Unreinforced Heat Resistant Information provided by Samsung Cheil Industries. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D1525 |
Dow DOWLEX™ 2025G Linear Low Density Polyethylene DOWLEX™ 2025G is a medium modulus resin with excellent toughness properties designed for thin film applications.Information provided by Dow |
|||
Vicat Softening Point | 113 °C | 235 °F | |
Dow Elite® 5110 Linear Low Density Polyethylene 5110 enhanced polyethylene resin is a copolymer produced via INSITE Technology from Dow Plastics. It offers unique combination of high modulus and excellent impact strength, allowing for downgaugin.. |
|||
Vicat Softening Point | 113 °C | 235 °F | |
Dow Tyril® 125 SAN Dow TYRIL® 125 resin is specially formulated for blending and is an ideal carrier material for use in making color concentrates. It offers high melt flow and excellent chemical resistance.Data prov.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D1525 |
Engineered Plastics EP Alloy 510B PC/ABS Alloy Gray. Stiff tough and excellent color stability. Used in housings for computers, printers, copiers and for auto parts such as air ducts and instrument panels. GMP # 002; Ford # WSS585. Propert.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Method B; ASTM D-1525 |
Bhansali Engineering Abstron KU-600 ABS Super Heat Resistant High Heat Resistant Grades with Better Flow characteristicInformation provided by Bhansali |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite Optix® CP - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite Optix® CP - 80 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Vicat Softening Point | 113 °C | 235 °F | ASTM D-1525 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Vicat Softening Point | 113 °C | 235 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Cycoloy® CX1440 PC+ABS (Asia Pacific) CYCOLOY CX1440 is a general purpose PC+ABS blend specially developped for thin wall applications requiring weld line strength and high flow with a good balance of properties |