Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin  (Unverified Data**)

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional molding equipment.Measured on 102mm x 102mm x 3.2 mm plaques, edge gated.Information provided by Chevron PhillipsSolvay Specialty Polymers has acquired the Ryton product line.
Physical Properties Metric English Comments
Density 1.95 g/cc
0.0704 lb/in³
ISO 1183A
Water Absorption 0.020 %
0.020 %
ASTM D-570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
0.0020 in/in
Linear Mold Shrinkage, Transverse 0.0050 cm/cm
0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 140 MPa
20300 psi
ISO 527
Elongation at Yield 1.0 %
1.0 %
ISO 527
Flexural Strength 215 MPa
31200 psi
ISO 178
Flexural Modulus 18.0 GPa
2610 ksi
ISO 178
Compressive Strength 270 MPa
39200 psi
ISO 604
Izod Impact, Notched (ISO) 6.00 kJ/m²
2.86 ft-lb/in²
ISO 180A
Izod Impact, Unnotched (ISO) 18.0 kJ/m²
8.57 ft-lb/in²
ISO 180A
Thermal Properties Metric English Comments
CTE, linear 15.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
8.33 µin/in-°F

@Temperature -58.0 - 122 °F
Axial; ISO 11359-2
15.0 µm/m-°C

@Temperature 100 - 200 °C
8.33 µin/in-°F

@Temperature 212 - 392 °F
Axial; ISO 11359-2
CTE, linear, Transverse to Flow 30.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
16.7 µin/in-°F

@Temperature -58.0 - 122 °F
ISO 11359-2
70.0 µm/m-°C

@Temperature 100 - 200 °C
38.9 µin/in-°F

@Temperature 212 - 392 °F
ISO 11359-2
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
ISO 75
UL RTI, Electrical 220 - 240 °C
428 - 464 °F
UL 746B
Flammability, UL94 5VA
5VA
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
ASTM D-257
Insulation Resistance 1.00e+11 ohm
1.00e+11 ohm
90°C, 95% RH, 48 hr
Dielectric Constant 4.8

@Frequency 1000 Hz
4.8

@Frequency 1000 Hz
ASTM D-150
4.8

@Frequency 1e+6 Hz
4.8

@Frequency 1e+6 Hz
ASTM D-150
Dielectric Strength 16.0 kV/mm
406 kV/in
ASTM D-149
Dissipation Factor 0.0010

@Frequency 1e+6 Hz
0.0010

@Frequency 1e+6 Hz
ASTM D-150
0.0020

@Frequency 1000 Hz
0.0020

@Frequency 1000 Hz
ASTM D-150
Arc Resistance 180 sec
180 sec
ASTM D-495
Comparative Tracking Index 250 V
250 V
UL 746A
Processing Properties Metric English Comments
Melt Temperature 315 - 345 °C
599 - 653 °F
Mold Temperature 135 °C
275 °F