Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem 2200N PEI (Europe-Africa-Middle East) 20% Glass fiber filled Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210F PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM 2210K PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Europe-Africa-Middle East) VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific) PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® ENH4565 PBT (Asia Pacific) 33% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin, Good thermal shock resistance and low CTE. |
|||
Tensile Strength, Yield | 140 MPa @Strain 0.200 %, Temperature 300 °C |
20300 psi @Strain 0.200 %, Temperature 572 °F |
Annealed prior to test |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® NH-3402F PC, 40% Glass Filled FR PC/GF material with 40% GF reinforcement that can be used in printer LSUInformation provided by Samsung Cheil Industries. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | SABIC - Japan Method |
SABIC Innovative Plastics NORYL GTX CRN530 PPE+PA6 (Asia Pacific) 30%GF GTX grade for Non Auto market |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Asia Pacific) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GTX GTX8720 PPE+PA (Europe-Africa-Middle East) Noryl GTX* GTX8720 resin is a glass filled, high performance blend of PPE/PA that exhibits an excellent balance of high-heat resistance, strength, flow, and conductivity. This grade can be electro-.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ASTM D638 |
Techmer ES Plastiblend® PA6 GF20 RM-B L NAT Nylon 6 Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAdditive: LubricantFeatures: Low Moisture Absorption and LubricatedAppearance: BlackTPCI.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ASTM D638 |
Solvay TECHNYL® 2417IG PA66, 20% glass fiber, DRY Description: Polyamide 66, 20% glass fiber reinforced, Impact modified for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® 2417IG4 is used in all sectors of industries,.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ASTM-D638 |
Polyram Polytron P60B04 Homopolymer Polypropylene, Chemically Coupled 60% Long Glass Fiber A CHEMICALLY COUPLED PP 60% LONG GLASS FIBER WITH EXTRA LOAD OF ADDITIVES FOR DILUTION.Information provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ISO 527 |
Polyram RamSter PF310G6 PBT Alloy, 30% Glass Fiber, UV Stabilized 30% Glass fiber reinforced PBT alloy, low warp properties, UV stabilized for injection molding.Information provided by Polyram. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ASTM-D638 |
Polyram RamSter PF321G6 PBT, 30% Glass Fiber, Flame Retardant 30% Glass fiber reinforced, flame retardant PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® KR 4365 G5 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® KR 4365 G5 BK 00100 35% Glass Filled PA6/6T FR (Conditioned) Description: Partially aromatic polyamide; flame retardant based on red phosphorus; low water absorption, high melting point (295°C); low tendency to form deposits on electrical contacts, very resi.. |
|||
Tensile Strength, Yield | 140 - 240 MPa | 20300 - 34800 psi | |
ArcelorMittal 02 High formability steel for drawing, Cold rolled Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used extensively in the automotive industry, both for visible and stru.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 50mm/min; ISO 527-2 |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Tensile Strength, Yield | 140 - 180 MPa | 20300 - 26100 psi | |
ArcelorMittal 05 High formability steel for drawing, Cold rolled Available in the following: uncoated (DC05) and electroglavanized (DC05+ZE) Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These product.. |
|||
Tensile Strength, Yield | 140 - 240 MPa | 20300 - 34800 psi | |
ArcelorMittal 52 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX52D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |
|||
Tensile Strength, Yield | 140 - 240 MPa | 20300 - 34800 psi | |
ArcelorMittal 55+AS Aluminized steel Use: Very difficult drawing, 600°< T < 800°CInformation provided by ArcelorMittal |
|||
Tensile Strength, Yield | 140 - 180 MPa | 20300 - 26100 psi | |
ArcelorMittal 56 High formability steel for drawing, Cold rolled Available in the following: Extragal®/Galvannealed (DX56D +Z/+ZF)Description: This range of non-alloyed mild steels is designed for deep and extra deep drawing applications. These products are used.. |
|||
Tensile Strength, Yield | >= 140 MPa | >= 20300 psi | ASTM-D638 |
Polyram PlusTek RA320G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | >= 140 MPa | >= 20300 psi | ASTM-D638 |
Polyram PlusTek RA321G6 Nylon 6.6, 30% Glass Fiber, Flame Retardant 30% glass fiber reinforced, flame retardant polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | ISO 527 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |
|||
Tensile Strength, Yield | 140 MPa | 20300 psi | 50 mm/min; ISO 527-2 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |