Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.95 g/cc | 0.0704 lb/in³ | |
3M Dyneon™ THV™ 200G Fluorothermoplastic, Pellet Form
(discontinued **) Data provided by the manufacturer, Dyneon LLC.This unique, melt-processable, tetrafluoroethylene, hexafluoropropylene, and vinylidene fluoride (THV) terpolymer provides a unique combination of perf.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183A |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-120BL Polyphenylene Sulfide Compound
(Unverified Data**) Black Polyphenylene Sulfide CompoundRyton® R-7-120BL is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good weldline strength and low maintenance molding using.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | Apparent |
Gouda Vuurvast C Dense Refractory Brick Description: A dry-pressed fireclay brick for use up to 1250°C with a good resistance to acid slags and vapors. Application: industrial furnaces, chimneys, electrolytic reduction cells.Remarks: T.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | typical |
Momentive Performance Materials HBC Hot-Pressed Boron Nitride Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO R 1183 |
Multibase Multibatch® ME 50062 Anti-blocking Masterbatch LDPE. 80% CaCO3FilledVery Highly FilledInformation provided by Multibase |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP ZX06323 PPE+HIPS (Asia Pacific) This material is mineral filled PPO grade with high dielectric constant and low loss tangent |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp OFJ66 PPS - Linear (Asia Pacific) LNP* Thermocomp* OFJ66 is a compound based on PPS - Linear resin containing Glass Fiber, Mineral. Added features of this material include: Low Warpage.This data was supplied by SABIC-IP for the Asi.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America FS-10-VO-P Short-Glass Reinforced Diallyl Phthalate Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type SI.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America SI 9045C Silicone Compound Long fiberglass and graphite filled silicone molding compound which offers moderate strength properties, high impact resistance, and excellent thermal stability at elevated temperatures.Information .. |
|||
Density | 1.95 - 2.06 g/cc | 0.0704 - 0.0744 lb/in³ | ASTM D792 |
Zeus THV Tubing THV Tubing is a Terpolymer of Tetrafluoroethylene, Hexafluoropropylene and Vinylidene fluoride. THV is the most flexible fluoropolymer available and has the highest degree of optical clarity. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax B Phenolic, Glass Fabric Reinforcement, Dark Brown, Sheet High performance/price ratio insulation material. Self-extinguishing, halogen-free, very low smoke emission and toxicity. Mechanically much stronger than the Etronit and Etronax types.Information pr.. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | 24hr/23°C/50% RH; ISO 1183-A; IEC/EN 60893-2 8.1 |
Elektro-Isola G-Etronax PI Polyimide, Glass Fabric Reinforcement, Dark Brown, Sheets Description: The most temperature-resistant material of all types. Retains its outstanding mechanical properties even at very high application temperatures. Applications: Used as thermal insulation .. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | |
Aremco Aremco-Bond™ 2315X High Temperature Epoxide Potting Compound Improved Crack Resistance & Bond Strength. High Temperature Resistance, Thermally Conductive, Low Viscosity. |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | Relative Density; ASTM D792 |
Sumitomo Bakelite North America TEM 9053C Hardware Grade Epoxy Short fiberglass and mineral filled, toughened epoxy molding compound with excellent dimensional stability and high strength properties.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.95 g/cc | 0.0704 lb/in³ | ASTM D792 |
Quantum Composites QC-8805 66% Glass Fiber Vinyl Ester SMC
(discontinued **) QC-8805 is a vinyl ester-based sheet molding compound (SMC) reinforced with continuous, unidirectional (0°) glass fibers. It provides high strength, stiffness, and fatigue resistance in the fiber .. |