Thermal Conductivity 0.580 - 0.580 W/m-K

@Temperature 100 - 100 °C
4.03 - 4.03 BTU-in/hr-ft²-°F

@Temperature 212 - 212 °F
Average value: 0.580 W/m-K Grade Count:1
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum ..
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Ryton® R-7-121BL Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
ASTM C177
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide (PPS), GlassMineral Filled
Ryton® R-7-121NA and R-7-121BL glass fiber and mineral filled polyphenylene sulfide compounds provide good mechanical strength with good flow and low maintenance molding using conventional moldin..
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
ASTM C518
Sumitomo Bakelite North America RX® 431 Cellulose Reinforced Phenolic Novolac
RX431 is a cellulose fiber reinforced phenolic novolac molding compound. This material is recommended for large parts requiring moderate toughness. It is designed to meet the requirements of ASTM D..
Thermal Conductivity 0.580 W/m-K

@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 00755 Melamine-Phenolic, Granular, Compression Molded
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755..
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Thermal Conductivity 0.580 W/m-K

@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 6990 Phenolic, Briquette, Transfer Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
Trelleborg Emerson & Cuming Stycast® 2651-1 One-Component Epoxy High Service Temp Encapsulant
Features and Typical ApplicationsAbility to withstand high temperatures, thermal shock, and chemical exposure. These products are designed for heat generating electronic devices which operate in har..
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
Trelleborg Emerson & Cuming Stycast® E-1030 One-Component Epoxy Low Stress Encapsulant
Emerson & Cuming E-1030 Stycast® One-Component Epoxy Low Stress EncapsulantDesigned for the encapsulation of a wide range of stress sensitive electronics. They offer excellent performance at low te..
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
Moulding Direction; ASTM C177
Dalau Dalcon 021 75% Virgin PTFE, 25% Carbon Coke
Applications & Industries: General: Carbon / Coke (soft) filler is good in dry running conditions, adds to the creep resistance, increases the hardness and raises the thermal conductivity of PTFE; C..
Thermal Conductivity 0.580 W/m-K

@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 00714 Melamine-Phenolic, Granular, Transfer Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Thermal Conductivity 0.580 W/m-K

@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Plenco 7552 Phenolic, Nodular, Injection Molded
PLENCO 07552 is a glass fiber reinforced novolac phenolic molding compound, exhibiting superior dimensional stability, good impact strength, and good electrical properties. Type ASTM 5948 MFH. UL re..
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
ASTM F433
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac
RX 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bak North America.
Thermal Conductivity 0.580 W/m-K
4.03 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin  (Unverified Data**)
Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi..