Dow Corning 3-4207 DIELECTRIC TOUGH GEL KIT

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3-4207 DIELECTRIC TOUGH GEL KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, translucent green, fast RT or heat cure, tough, primerless chemical adhesion, UV indicator, and UL 94 V-1 flammability classification.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc

@Temperature 25.0 °C
0.980 g/cc

@Temperature 77.0 °F
Viscosity 430 cP
430 cP
dynamic
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 7.10e+13 ohm-cm
7.10e+13 ohm-cm
Dielectric Constant 2.85

@Frequency 100 Hz
2.85

@Frequency 100 Hz
2.86

@Frequency 100000 Hz
2.86

@Frequency 100000 Hz
Dielectric Strength 16.5 kV/mm
420 kV/in
Dissipation Factor <= 0.00010

@Frequency 100000 Hz
<= 0.00010

@Frequency 100000 Hz
0.030

@Frequency 100 Hz
0.030

@Frequency 100 Hz
Processing Properties Metric English Comments
Cure Time 3.00 min

@Temperature 100 °C
0.0500 hour

@Temperature 212 °F
5.00 min

@Temperature 75.0 °C
0.0833 hour

@Temperature 167 °F
10.0 min

@Temperature 50.0 °C
0.167 hour

@Temperature 122 °F
15.0 - 90.0 min

@Temperature 22.0 °C
0.250 - 1.50 hour

@Temperature 71.6 °F
Shelf Life 6.00 Month
6.00 Month
Descriptive Properties Value Comments
Appearance translucent
Color green
Flowable yes
Gel Hardness (Grams/Penetration) 9490
Hydrophobic yes
Self Leveling yes
Water Resistant yes
Working Time (min) 10