Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 220 °C | 428 °F | per UL Card E54153 |
Arlon 48571R005 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |
|||
UL RTI, Electrical | 220 °C @Thickness 0.750 mm |
428 °F @Thickness 0.0295 in |
|
Solvay Specialty Polymers Xydar® G-930 Liquid Crystal Polymer (LCP), 30% Glass Fiber Xydar® G-930 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electrical/electronic applications utilizing surface mount technology.The moldab.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Card E54153 |
Arlon 30570XA015 0.015" (0.381mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. Th.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 32570R040 0.040" (1.02 mm) Uncured Silicone Rubber with Fiberglass Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Card E54153 |
Arlon 48576R005 0.0055" (0.140 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specific.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55572AA024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass This data represents typical values for the production material. The data should not be us.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55572XA028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55578R030 0.0325" (0.825 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1, Layer 2: Uncured Silicone Rubber Side 1, Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Side 2: Cured Silicone Rubber Appearance:.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL card E54153 |
Arlon 55579R028M 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured layer on top of a cured layer on one side This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | File E54153 |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | |
Arlon CP-410R Bulk Compound Design/Construction: Bulk Compound (packaged in polyethylene) This data Represents typical values for the production material. The data should not be used to write, or in place of, material specific.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL card E54153 |
Arlon R34931R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Car E54153 |
Arlon 44571B010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Car E54153 |
Arlon 44571R010A 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Car E54153 |
Arlon 44576R016 0.016" (0.406 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | File E54153 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | |
Arlon 51576R016A 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL card E63753 |
Arlon 51576X015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55276B028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data represents typical values for the production mate.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL card E54153 |
Arlon 55578XA030M 0.0305" (0.775 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | |
Arlon CP-427R Silicone Rubber bulk compound |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL card E63753 |
Arlon R31678R016 0.0175" (0.444 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone/Kapton Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass cloth with Kapton® film on opposite side.This data Represents typical va.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | per UL Car E54153 |
Arlon 44570B010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specificati.. |
|||
UL RTI, Electrical | 220 °C | 428 °F | E54153 |
Arlon 48981R010 0.0100" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 3 mil PolyethyleneSide 1: Uncured RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave 2: 3 mil PolyethyleneThis data represents typic.. |