Tra-Con Tra-Bond 724-5 Low Viscosity Polyurethane Adhesive

Category Polymer , Adhesive , Thermoset , Polyurethane, TS
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 724-5 Low Viscosity Polyurethane Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 724-5 is a premixed and frozen, electrically insulating, polyurethane adhesive. This resilient adhesive exhibits good adhesion to a wide variety of substrates, including aluminum, solder, nylon, mylar, and steel. This resilient adhesive can also be used for tacking wires and as a protective coating.Information provided by Tra-Con Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Adhesive Bond Strength 15.2 MPa
2200 psi
Lap shear, alum to alum, 3 hrs @ 74°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 125 °C
257 °F
Continuous
125 °C
257 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+11 ohm-cm
2.00e+11 ohm-cm
cured 3 hrs @ 74°C
Dielectric Constant 6.5

@Frequency 1000 Hz
6.5

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 74.0 °C
3.00 hour

@Temperature 165 °F
preferred
480 min

@Temperature 60.0 °C
8.00 hour

@Temperature 140 °F
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Shelf Life 1.00 Month

@Temperature -40.0 °C
1.00 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Working Life minutes 30
At 25°C