Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 315 - 325 °C | 599 - 617 °F | Optimum adhesion is obtained at a draw span of about 10 cm. Treatment of the substrate or the use of primers will significantly enhance adhesion. |
NOVA Chemicals Novapol® LC-0517-A LDPE Extrusion Resin Excellent adhesion, High drawdown, Excellent sealabilityApplications: Dry soup pouches, Powdered drink pouches, Pharmaceutical packaging, Potato chip bags, Flexible and snack food packagingAdditives.. |
|||
Melt Temperature | 315 - 325 °C | 599 - 617 °F | Optimum adhesion is obtained at a draw span of about 10 cm. Treatment of the substrate or the use of primers will significantly enhance adhesion. |
NOVA Chemicals Novapol® LC-0522-A LDPE Extrusion Resin Excellent sealability, High drawdown, High adhesion, Good barrier, High stiffness, Good abrasion resistanceApplications: Milk cartons, Paperboard containers, Liquid packaging, Woven fabrics, Lumber .. |
|||
Melt Temperature | 315 - 325 °C | 599 - 617 °F | Optimum adhesion is obtained at a draw span of about 10 cm. Treatment of the substrate or the use of primers will significantly enhance adhesion. |
NOVA Chemicals Novapol® LC-0717-A LDPE Extrusion Resin High speeds, Low coating weights, Excellent adhesion, Excellent drawdown, Excellent sealabilityApplications: Sugar pouch stock; Popsicle wrap, Multi-wall bags, High speed/low coating weight paper co.. |
|||
Melt Temperature | 315 - 325 °C | 599 - 617 °F | Extrusion Coating |
NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin
(discontinued **) Features: Octene co-polymer, excellent sealability and toughness, high drawdown, high adhesion, good barrier, good abrasion resistance.Applications: Food packaging, milk cartons, paperboard containe.. |
|||
Melt Temperature | 315 - 325 °C | 599 - 617 °F | |
NOVA Chemicals Novapol® LE-0520-AM LDPE Extrusion Resin
(discontinued **) Features: easy processing, good dispersion.Applications: extrusion coating.Data provided by the manufacturer. |
|||
Melt Temperature | 315 - 325 °C | 599 - 617 °F | |
NOVA Chemicals Novapol® LM-1019-A LDPE Masterbatch Resin
(discontinued **) Features: easy processing, good dispersion.Applications: masterbatch/compounding.Data provided by the manufacturer. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Solvay Specialty Polymers Ryton® R-7-220BL Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Chevron Phillips Xtel® XE3200NA Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XE3200NA is an un-reinforced high performance, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information provided b.. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Chevron Phillips Xtel® XE5300NA Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XE5300NA is a high performance extrusion grade PPS based alloy developed to provide excellent mechanical strength, elongation and chemical resistance.Information provided by Chevron Phillips |
|||
Melt Temperature | 315 °C | 599 °F | Resin, Injection Molding |
LG Chemical LUCON SP9306FL sPS+MF Description Injection Molding Grade, sPS+MF, Low Thermal Conductivity, Chemical Resistance, High Heat ResistanceApplication: Electrical or Electronic Parts CAS No. 9003-53-6, 65997-17-3, 68928-70-1 .. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Chevron Phillips Xtel® XE3035BL Polyphenylene Sulfide Alloy Xtel® XE3035BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Chevron Phillips Xtel® XE4050BL Polyphenylene Sulfide Alloy Xtel® XE4050BL is a glass fiber and mineral filled PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevron Phillips.. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Chevron Phillips Xtel® XE5030BL Polyphenylene Sulfide Alloy Xtel® XE5030BL is a high performance, glass fiber reinforced, PPS based alloy developed to provide high ductility and impact strength along with good thermal stability.Information provided by Chevr.. |
|||
Melt Temperature | 315 - 332 °C | 599 - 630 °F | Extrusion Coating Processability |
Dow 4010 Low Density Polyethylene (LDPE) Polyethylene 4010 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry and moist foods packaging, sugar pouches, lidding stoc.. |
|||
Melt Temperature | 315 - 327 °C | 599 - 621 °F | Extrusion Coating Processability |
Dow 4012 Low Density Polyethylene (LDPE) Polyethylene 4012 is used for a variety of applications such as condiment packaging, dry and moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow |
|||
Melt Temperature | 315 - 332 °C | 599 - 630 °F | Extrusion Coating Processability |
Dow 722 Low Density Polyethylene (LDPE) Polyethylene 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist foods pac.. |
|||
Melt Temperature | 315 - 320 °C | 599 - 608 °F | |
Eurostar Starglas OC004 PPS, 20% Carbon Filled, Injection Molded Starglas OC004 is a 20% Carbon Fiber Reinforced PPS Injection Molding ResinInformation provided by Eurostar. |
|||
Melt Temperature | 315 °C | 599 °F | Optimal |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Melt Temperature | 315 °C | 599 °F | Optimal |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Melt Temperature | 315 - 345 °C | 599 - 653 °F | |
Solvay Specialty Polymers Ryton® R-7-121NA Polyphenylene Sulfide Resin
(Unverified Data**) Ryton® R-7-121NA is an advanced glass/mineral filled polyphenylene sulfide compound developed to provide good mechanical strength with good flow and low maintenance molding using conventional moldi.. |