Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP LUBRICOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP LUBRICOMP RFN18 PA 66 (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP* Lubricomp* RFN18 is a compound based on Nylon 66 resin containing Glass Fiber, MOS2.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.0015 - 0.0035 cm/cm
0.0015 - 0.0035 in/in
on Tensile Bar; SABIC Method
Mechanical Properties Metric English Comments
Tensile Strength at Break 221 MPa
32100 psi
5 mm/min; ISO 527
Elongation at Break 2.4 %
2.4 %
5 mm/min; ISO 527
Tensile Modulus 14.5 GPa
2100 ksi
1 mm/min; ISO 527
Flexural Strength 306 MPa
44400 psi
2 mm/min; ISO 178
Flexural Modulus 11.4 GPa
1650 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 80.0 kJ/m²
38.1 ft-lb/in²
80*10*4; ISO 180/1U
Coefficient of Friction, Dynamic 0.75
0.75
ASTM D3702 Modified
Coefficient of Friction, Static 0.59
0.59
ASTM D3702 Modified
K (wear) Factor 90.6 x 10-8 mm³/N-M
45.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 262 °C
504 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
Deflection Temperature at 1.8 MPa (264 psi) 251 °C
484 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af