Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Quantum Composites QC-8777 41% Glass Fiber Reinforced Polyester Hybrid SMC QC-8777 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength, corrosion resistance and temperature.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
LNP Lubricomp® OFL-4536 Polyphenylene Sulfide, Glass Fiber Reinforced, PTFE Lubricant
(discontinued **) Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-8930 HS Polyphthalamide (PPA), 30% Glass Fiber Amodel® A-8930 HS is a 30% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® AE-1133 Polyphthalamide (PPA), 33% Glass Fiber Amodel® AE-1133 is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) designed to work in the modern automotive electrical environment. It has a high heat deflection temperature, high .. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP CF008 PS LNP* THERMOCOMP* CF008 is a compound based on Polystyrene resin containing 40% Glass Fiber. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069SZ PA 66 LNP* THERMOCOMP* RF0069SZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of th is grade include: Flame Retardant, Heat Stabilized. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Conditioned) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resist.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXAMID 126F10 Nylon 6, 50% Glass Fiber SAXAMID 126F10 is a polyamide 6 injection-molding-grade reinforced with 50% glass fibers.Information provided by SAX Polymers |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ISO 178 |
Polyram PlusTek PB318G9 Nylon 6 for Injection Molding, 45% Glass-fiber Reinforced, UV Stabilized 45% Glass-fiber reinforced Nylon 6, UV stabilized for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ISO Data |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ASTM D790 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Flexural Modulus | 11.4 GPa @Temperature 23.0 °C |
1650 ksi @Temperature 73.4 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® A-6135 HN Polyphthalamide (PPA)
(Unverified Data**) Amodel A-6135 HN polyphthalamide (PPA) is a 35% glass reinforced resin that is heat stabilized, lubricated and hot-water moldable. Key properties of the resin are high heat resistance, high strength.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | ISO 178 |
Solvay Specialty Polymers Amodel® A-6135 NL Polyphthalamide (PPA), 35% Glass Fiber Reinforcement
(discontin Amodel A-6135 NL polyphthalamide (PPA), a 35% glass reinforced, high-glow, non-lubricated, hot-water moldable resin specially designed for laser welding. The black version is a laser absorber, and t.. |
|||
Flexural Modulus | 11.4 GPa | 1650 ksi | 5 mm/min; ISO 178 |
Gromax CFG45-RN13N1 Nylon 6 46% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |