Ineos HP54-60 Flake Polyethylene Copolymer Flake

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos HP54-60 Flake Polyethylene Copolymer Flake.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a high density polyethylene copolymer flake which contains no additives and is not pelletized. It is designed for use in the plastic wood composite market.Information provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Density 0.954 g/cc
0.0345 lb/in³
ASTM D4883
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 24.1 MPa
3500 psi
2 in/min; ASTM D638
Elongation at Break >= 600 %
>= 600 %
2 in/min; ASTM D638
Tangent Modulus >= 1030 MPa
>= 150000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 68.3 °C
155 °F
ASTM D648
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding