Tra-Con Tra-Bond 216C03 Flexible Plastic Bonder

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 216C03 Flexible Plastic Bonder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 216C03 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermoplastic substrate. TRA-BOND 21C03 is low viscosity and easy to apply. It has an easy 1:1 mix ratio and can be cured at room temperature. This high technology system was formulated for applications in the automotive, medical, aerospace, photonic and assembly industries and can be used anywhere that requires excellent chemical fastening to plastic parts. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
Cured
Viscosity 16000 cP
16000 cP
Mixed (lv #4, 12 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
1 hr @ 65°C
90
90
24 hrs @ 25°C
Adhesive Bond Strength 7.24 MPa
1050 psi
Lap shear, alum to alum, 24 hrs @ 25°C
10.3 MPa
1500 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 18.0 °C
64.4 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Amber
Cured
Mix Ratio, parts by weight 1/1
Resin/Hardener