Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0015 - 0.0020 cm/cm | 0.0015 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ AS-15CF/000 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | ISO 294-4 |
Polyplastic Armamid® PA GF25-1FR Nylon 6, 25% Glass Fiber Flame retardant, RoHS compliantInformation provided by PolyPlastic Group. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | ASTM D955 |
PolyOne Edgetek® NY-20CF/000 BLACK Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® LCG2007 PC (Asia Pacific) |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP AFP26 ABS (Europe-Africa-Middle East) LNP* Lubricomp* AFP26 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, PTFE, Silicone. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0035 cm/cm | 0.0015 - 0.0035 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP RFN18 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN18 is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Ultem 3451 PEI (Asia Pacific) 45% Glass fiber and mineral filled, standard flow Polyetherimide (Tg 217C) with enhanced dimensional stability. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES Electrablend® ABS CF20 BK 20% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | |
Solvay Specialty Polymers Kalix® 2855 Polyamide, High Performance (HPPA), Glass Fiber Kalix® 2855 is a 27% bio-sourced, PA 6,10-based compound with 55% by weight glass fiber reinforcement. This material is formulated to provide maximum strength, stiffness, impact resistance, and p.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0030 cm/cm @Time 86400 sec |
0.0015 - 0.0030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP LC006EXQ PEEK LNP* THERMOCOMP* LC006EXQ is a compound based on Polyetheretherketone containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Time 86400 sec |
0.0015 - 0.0025 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Thermocomp RF0057E PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF0057E is a compound based on Nylon 66 resin containing Glass Fiber, Flame Retardant. Added features of this material include: Non-Brominated & Non-Chlorinated Flame Retardant.Thi.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF20 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackTPCI# 9822121Information provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS GF20 LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 3.17 mm |
0.0015 in/in @Thickness 0.125 in |
ASTM D955 |
Techmer ES HiFill® ABS IM TM20 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingInformation p.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP 9X94104 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* 9X94104 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | GB/T 15585-1995 |
Sichuan Deyang Haton® hMR61 Polyphenylene Sulfide, Glass & Mineral Reinforced Injection moldingInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP NF0061 PC+ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* NF0061 is a compound based on PC+ABS resin containing Glass Fiber, Flame Retardant. Added features include : Flame Retardant. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm @Thickness 6.40 mm |
0.0015 in/in @Thickness 0.252 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Noryl_FM4025 PPE+PS LNP* Thermocomp* Noryl_FM4025 compound is GR/MR 40%, high modulus structural foam. 10% weight reduction, 0.250"" wall thickness. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp OC004 PPS - Linear (Europe-Africa-Middle East) LNP* THERMOCOMP* OC004 is a compound based on PPS-Linear resin containing Carbon Fiber. Added features include : Electrically Conductive.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP OF008A PPS - Branched (Europe-Africa-Middle East) LNP* Thermocomp* OF008A is a compound based on PPS - Branched resin containing Glass Fiber. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP Thermocomp ZF004XXC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004XXC is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm @Thickness 3.20 mm |
0.0015 - 0.0025 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL CN5258 PPE+PS (Asia Pacific) 40% filled FR high modulus PPE/PS blend |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | on Tensile Bar; E2P method |
Eurostar Staramide BG8 PA6, 40% Glass Fiber Filled, Injection Molded Staramide BG8 is a 40% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Linear Mold Shrinkage, Flow | 0.0015 cm/cm | 0.0015 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOTUF OF008EI PPS (Europe-Africa-Middle East) LNP* Thermotuf* OF008EI is a compound based on PPS-Linear resin, containing Glass Fiber. Added features include : High Impact and Easy Molding. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0030 cm/cm | 0.0015 - 0.0030 in/in | |
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Linear Mold Shrinkage, Flow | 0.0015 - 0.0025 cm/cm | 0.0015 - 0.0025 in/in | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |