Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 221 MPa | 32100 psi | 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ NN-40CF/000 FRV0 Natural Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | ASTM D638 |
Niche Polymer PA66GF43BK Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | ASTM D638 |
Niche Polymer PA66GF43N Nylon 66, 43% Glass Fiber Filled Information provided by Niche Polymer |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NN-40CF/000 FRV0 NATURAL Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 1200 A 43 HS Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GF 1200 A 43 Natural Polyamide 66 (Nylon 66) The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil.. |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater than 0.. |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | ISO 527-1/-2 |
Lanxess Durethan® DP AKV 50 HR H2.0 901510 Nylon 66, 50% Glass Fiber PA 66, injection molding grade, 50% glass fibers, good heat-ageing resistance, and hydrolysis resistanceApplication Examples: coolant manifolds |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFN18 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFN18 is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) resin that provides excellent structural integrity in molded parts, even those with wall thicknesses greater th.. |
|||
Tensile Strength at Break | 221 MPa | 32100 psi | ASTM D638 |
Solvay Specialty Polymers Amodel® AS-1933 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-1933 HS is a 33% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material excee.. |