ExxonMobil Paxon™ AD60-007 Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Exxon Chemical
Trade Name Paxon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Paxon™ AD60-007 Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: AD60-007 is a medium molecular weight distribution high-density polyethylene homopolymer. It possesses excellent processing uniformity and produces bottles with excellent appearance and rigidity. AD60-007 offers the maximum in barrier properties available in high-density polyethylene, and imparts minimum odor and taste to the packaged product.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: No Applications: Food packagingLiquid Food Containers for Milk, Water and Juices Thermoformed Parts Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.963 g/cc
0.0348 lb/in³
ASTM D4883
ESCR 100% Igepal® 10 hour
10 hour
ASTM D1693 Condition B
Melt Flow 0.73 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.73 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.4 MPa
4700 psi
ASTM D638
Elongation at Break 350 %
350 %
ASTM D638
Flexural Modulus 1.72 GPa
250 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 126 kJ/m²
60.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
260 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F