Polymer Property : Density = 0.0556 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Celanese Celanex® 3309HR PBT, 30% Glass Reinforced  (Unverified Data**)
Celanex 3309HR is a non-lubricated, 30% fiberglass reinforced Polybutylene Terephthalate which has excellent hydrolysis resistance, mechanical properties and processability.30% glass reinforced, hyd..
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Celanese Celstran® PBT-GF30-08 PBT, 30% Glass Reinforced  (Unverified Data**)
30% Long Glass Fiber Reinforced PBT30% Long Glass Fiber Reinforced PBTCelstran can be processed on a standard injection molding unit.Information provided by Celanese
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Celanese Hostaform® C 9021 GV1/30 GT POM, 26% Tribological  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POM26% glass fiber reinforced, specialty low wear grade based on UHMWPEInformation provided by Celanese
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183/A
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, DRY
Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:..
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
SABIC Innovative Plastics LNP LUBRICOMP UFL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UFL36AS is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE. Added features include Internally Lubricated, Heat Stabilized.
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Techmer ES HiFill FR® PA6 GF25 FR HS L 25% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and Lu..
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific)
PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP JF004LZ PES
LNP* Thermocomp* JF004LZ is a compound based on PES containing 20% Glass Fiber. Added features include: Extrusion Grade, Low Extractible.
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Techmer ES HiFill® TPX-HTN-01033 A 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Heat StabilizerFeatures: Heat Stabilized and High Temperature StrengthUL File ..
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Plenco 3303 Phenolic, Granular, Injection Molded
Plenco 03303 is a renumber of Plaslok 5303. Plenco 03303 is a two-stage, mineral and flock-filled phenolic molding compound offering excellent electrical insulating properties. It can be processed b..
Density 1.54 g/cc
0.0556 lb/in³
GB/1033
Zhejiang Juner PA-A4 Flame-Retardant & Mineral Reinforced PA6
Applications: Top Grad CBInformation provided by Zhejiang Juner New Materials Co, Ltd.
Density 1.54 g/cc
0.0556 lb/in³
Toyobo Zylon® AS Poly(p-phenylene-2,6-benzobisoxazole) Fiber
Property data below is for 1.5 denier fiber. Poly(p-phenylene-2,6-benzobisoxazole) (PBO) is a rigid-rod isotropic crystal polymer. Zylon is a new high performance fiber developed by TOYOBO using t..
Density 1.54 g/cc
0.0556 lb/in³
(DAM); ISO 1183
DSM Stanyl® TW271F6 (COND) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America)
Information provided by DSM Engineering Plastics.
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry)
Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper..
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Ensinger XP-154 Compression Molded PI Compound, 40% Graphite, Premium Grade
The XP 150 Series are amorphous high performance polyimides with high permanent temperature and creep resistance, as well as excellent bearing and wear properties, and excellent long term thermal st..
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1183
Fainplast Compounds AP 80 Flexible PVC, Flame Retardant Insulation
General purposes
Density 1.54 - 1.58 g/cc
0.0556 - 0.0571 lb/in³
ISO R 1183
Fainplast Compounds GA 77/1 Flexible PVC, Flame Retardant Sheathing
General purposes
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Eurostar Starflam PK0049 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded
Starflam PK0049 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Eurotec® Tecodur® PB70 GR15 NL XA 20 PBT 15% glass fiber reinforced, UL94 V0
Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance..
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® SK615SF BK591 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF BK591 is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for i..
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Ensinger Tecaform™ HPV 13 Acetal Homopolymer - Extruded Products (POM)
Tecaform™ HPV 13 is a brown homopolymer acetal with an internal PTFE lubricant. Its low coefficient of friction, excellent PV values, toughness, wear resistance, and machinability make it an excep..
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Eurotec® Tecomid® NT40 MR40 NL HS PPA, 40% mineral reinforced, heat stabilized, natural
Information provided by Eurotec®
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Ashley Polymers Ashlene® P126 PBT Polyester, 30% Glass Reinforced
PBT polyester with 30% glass reinforcement.Data provided by the manufacturer
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
Celanese Celstran® PBT-GF30-08 PBT, 30% Glass Reinforced
30% Long Glass Fiber Reinforced PBTInformation provided by Celanese
Density 1.54 g/cc

@Temperature 23.0 °C
0.0556 lb/in³

@Temperature 73.4 °F
ASTM D792
Beijing Ranger Chem PBT-201-G20 Flame Retarding FR PBT
Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin..
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Plaslok 504 Black (INJ) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound  (discontinued **)&l
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu..
Density 1.54 g/cc
0.0556 lb/in³
ASTM D792
Solvay TECHNYL® 2210HS PA66, DRY
Description: Polyamide 66, unfilled, long-term stabilized, lubricated for injection molding.Available in: Asia Pacific Product Applications: TECHNYL® 2210HS is used in all sectors of industry, offe..
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
DSM Arnite® TB6 260 PBT-GB30
Density 1.54 g/cc
0.0556 lb/in³
ISO 1183
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti..