Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 2311 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2311 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide improved pourability characteristics for cold powder compression molding. UL recognized under component file E40654. 02311 is available in black or brown color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Water Absorption 0.35 %
0.35 %
ASTM D570
Linear Mold Shrinkage 0.0074 cm/cm
0.0074 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 85
85
ASTM D785
Tensile Strength, Ultimate 51.0 MPa
7400 psi
ASTM D638
Elongation at Break 0.69 %
0.69 %
ASTM D638
Tensile Modulus 8.30 GPa
1200 ksi
ASTM D638
Flexural Strength 73.0 MPa
10600 psi
ASTM D790
Flexural Modulus 7.50 GPa
1090 ksi
ASTM D790
Compressive Strength 203 MPa
29400 psi
ASTM D695
Poissons Ratio 0.35
0.35
ASTM D638
Shear Modulus 3.07 GPa
445 ksi
Calculated
Izod Impact, Notched 0.175 J/cm
0.328 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.196 J/cm²
0.933 ft-lb/in²
ASTM D256
Impact 100
100
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 64.0 µm/m-°C

@Temperature 40.0 - 130 °C
35.6 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 199 °C
390 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 167 °C
333 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 26.6 %
26.6 %
ASTM D2863
Shrinkage 0.32 %
0.32 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 5.30e+11 ohm-cm
5.30e+11 ohm-cm
ASTM D247
Dielectric Constant 5.5
5.5
ASTM D150
Dielectric Strength 10.0 kV/mm
254 kV/in
Short Time; ASTM D149
Dissipation Factor 0.060
0.060
ASTM D150
Arc Resistance 142 sec
142 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638