Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 73.1 MPa | 10600 psi | ASTM D790 |
PolyOne Geon™ Vinyl Packaging 2121 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 73.1 MPa | 10600 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion L0660 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | 73.1 MPa | 10600 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Molding 6957 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 73.0 MPa | 10600 psi | STN EN ISO 178 |
Plastcom SLOVAMID 6 HI Polyamide 6, Impacted FeaturesPA 6 with the content of thermoplastic elastomer. Impacted, for mouldings with high toughness either at low temperatures, suitable for external use, eg. ski shoes, sports and safety helmets.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | |
Plastcom SLOVAMID 6 HI/1 TLS PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Flexural Strength | 73.1 MPa | 10600 psi | Conditioned; ASTM D790 |
Solvay Specialty Polymers Amodel® AT-1002 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AT-1002 HS is a neat, toughened, heat stabilized polyphthalamide (PPA) resin that offers superior retention of properties after humid thermal aging; high impact at low temperature and better .. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
Kolon KOCETAL® LW301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 2 mm/min; ISO 178 |
Ineos ABS Lustran® Ultra 4000 PG ABS Pellets (a-methylstyrene-SAN-modified), Electroplating Grade Lustran® Ultra 4000 PG is electroplating grade with high heat resistance. It is used for the production of molded plastic articles. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing 20% PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP ZP001XXP PPE+PS LNP* LUBRICOMP* ZP001XXP is a compound based on PPE+PS resin containing 5% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing... |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC (Asia Pacific) LNP* Lubriloy* D20009P is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant,.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
Styrolution Novodur® E211 ABS Novodur E211 is a high heat extrusion grade and suitable for blow moldingInformation provided by Styrolution |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX6601 PPE+PA66 (Asia Pacific) PPE+PA Unfilled GTX |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D 790 |
SABIC Innovative Plastics Noryl INT1000 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 73.1 MPa | 10600 psi | ASTM D790 |
Chase Plastics CP Pryme® A300 BK General Purpose (Utility) ABS Molding Resin Information provided by Chase Plastics. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Flexural Strength | 73.0 - 76.0 MPa | 10600 - 11000 psi | ASTM D790 |
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Flexural Strength | 73.1 MPa | 10600 psi | ASTM D-790 |
Axiall LSS-8200 Rigid PVC, Extrusion Georgia Gulf LSS-8200 is a special purpose rigid PVC sheet extrusion compound designated for reduced smoke emission properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
Flexural Strength | 73.1 MPa | 10600 psi | ASTM D-790 |
Axiall 7765 Rigid PVC, Extrusion Georgia Gulf 7765 is a general-purpose indoor rigid PVC profile extrusion compound designed for applications requiring the following properties. 7765 carries an NSF standard 51 listing (for food zo.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GB4 POM 20% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 72.9 - 75.7 MPa | 10600 - 11000 psi | ASTM D790M |
DSM Somos® ProtoCast™ AF 19122 Antimony-free Liquid Photopolymer Product DescriptionDSM Somos® ProtoCast™ AF 19122 is an antimony-free liquid photopolymer specifically formulated for producing investment casting patterns.ApplicationsIdeal for use in foundry app.. |
|||
Flexural Strength | 73.1 MPa | 10600 psi | ASTM D790 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific) LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |