Master Bond UV15FL One Component, High Strength, Flexible UV Curable Epoxy

Category Polymer , Adhesive , Thermoset
Manufacturer Master Bond Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Master Bond UV15FL One Component, High Strength, Flexible UV Curable Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Master Bond UV15FL is a one component, high strength, low viscosity, flexible UV curable epoxy resin based polymer system for bonding, sealing, & coating with exceptionally high performance properties. Shrinkage upon cure is less than 3%, significantly lower than that exhibited by free radical types of UV curable compositions.
Physical Properties Metric English Comments
Viscosity 200 - 300 cP

@Temperature 23.0 °C
200 - 300 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Light Amber; Clear