Electrical Properties | Metric | English | Comments |
---|---|---|---|
Arc Resistance | 142 sec | 142 sec | ASTM D495 |
Owens Corning Glass Fiber Reinforced Acetal, 25 wt.% glass Data provided by the manufacturer, Owens Corning. |
|||
Arc Resistance | 142 sec | 142 sec | ASTM D495 |
Eastman EASTALLOY Polymer DA105, Natural Alloy
(discontinued **) General: All ISO tests are run @ 4-mm thickness with the exception of Impact Resistance, which is run @ 2-mm thickness. Comments: Properties reported here are typical of average lots. Eastman ma.. |
|||
Arc Resistance | 142 sec | 142 sec | ASTM D495 |
Plenco 2308 Phenolic, Granular, Injection Molded PLENCO 02308 is a general purpose organic filled phenolic molding compound, offering improved heat resistance and optimized cure properties. UL recognized under component file E40654. 02308 is avai.. |
|||
Arc Resistance | 142 sec | 142 sec | ASTM D495 |
Plenco 2311 Phenolic, Granular, Transfer Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |