Polymer Property : Density = 0.0513 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792, ISO 1183
Nilit Nilitop BT FR C3 Unfilled, Flame Retardant PBT
Description: Nilitop BT FR C3 is an unfilled, flame retardant PBT with halogens. The flame retardant does not contain PBB and PBDE, so it is compliant with the WEEE directive.Key characteristics: Go..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183-1
Quadrant EPP Techtron® HPV PPS + solid lubricant, bearing grade, extruded (ISO Data)
As a reinforced, internally lubricated PPS grade, Techtron HPV PPS demonstrates an excellent combination of properties including wear resistance, load-bearing capabilities and dimensional stability ..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 127UVE RD402 Acetal Homopolymer  (Unverified Data**)
Delrin® 127UVE RD402 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information pro..
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
Asahi Kasei Tenac® 5012 Acetal Homopolymer  (discontinued **)
Standard-flow grade, with reduced stiffness and increased elongation through addition of special polymers.Applications: Clips, fasteners, press-fit parts.This product is not a part of the standard p..
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS
LNP* LUBRICOMP* CBL36XXC is a compound based on Polystyrene resin containing 30% Glass Bead and 15% PTFE. Added features of this material include: Wear Resistant.
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Hexion Bakelite™ PF 2137 Phenolic Formaldehyde Resin, High Surface Quality, Dishwasher Proof  (discontinued **
Phenolic molding compound, inorganically/organically filled, glass fiber reinforced, increased heat resistance, minimal distortion, dish washer proof.Application areas: Iron heat shields, fittings f..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183/A
Grupo Repol Dinalon® B1S25 G30PV0 30% Glass Reinforced, V-0 Rated (Phosphorous) Nylon 6
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP WAL34 PBT
LNP* LUBRICOMP* WAL34 is a compound based on (PBT resin containing 15% PTFE, 20% Aramid Fiber. Added features of this material include: Wesr Resistant.
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
SABIC Innovative Plastics Ultem PW2200 PEI (Europe-Africa-Middle East)
20% Glass fiber filled, standard flow Polyetherimide (Tg 217°C). Product designed and certified for use in Potable Water applications. KTW, WRAS, ACS certified. NSF61 and W270 pending. US FDA and..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP QF008 PA 6/10 (Asia Pacific)
LNP* Thermocomp* QF008 is a compound based on Nylon 6/10 resin containing Glass Fiber.
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
SABIC Innovative Plastics LNP THERMOCOMP RF007H PA 66
LNP* Thermocomp* RF007H is a compound based on Nylon 66 containing glass fiber. Added feature includes: Healthcare.
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
SABIC Innovative Plastics LNP THERMOCOMP ZFM62P PPE+PS
LNP* THERMOCOMP* ZFM62P is a compound based on PPE+PS resin containing 10% Glass Fiber, 30% Mical. Added features of this material include: Exceptional Processing.
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
SABIC Innovative Plastics LNP VERTON RX06479 PA 66 (Asia Pacific)
LNP VERTON* RX06479 is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding.
Density 1.42 g/cc
0.0513 lb/in³
DuPont™ Kapton® 100HN Polyimide Film, 25 Micron Thickness
Film thickness 25 micron (1.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Available in thicknesses from 0.3 mil (7.5 µm) to 5 mil (125 µm).General..
Density 1.42 g/cc
0.0513 lb/in³
DuPont™ Kapton® 300FPC Polyimide Film, 75 Micron Thickness
Film thickness 75 micron (3.0 mil)All purpose polyimide film. Can be laminated, diecut, slit, formed, or adhesive-coated. Similar to Kapton® Type VN with improved bondability. Available in thick..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
EMS-Grivory Grivory® XE 4104 nat PA610-GF40
Product description: Grilamid XE 4104 natural is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw materia..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 300PE NC010A Acetal Homopolymer
Delrin® 300PE NC010A is a medium-high viscosity acetal homopolymer, an enhanced version with extremely low VOC emissions. It has improved processing thermal stability, good mechanical properties, a..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration ..
Density 1.42 g/cc
0.0513 lb/in³
DIN 53 479
Ensinger TECASINT 4201 SD Polyimide, Black, Carbon Fiber (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® PC691 NC010 Acetal (POM)  (Unverified Data**)
Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the health..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® SC690 NC010 Acetal (POM)  (Unverified Data**)
Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare indus..
Density 1.42 - 1.46 g/cc
0.0513 - 0.0527 lb/in³
ISO R 1184
Fainplast Compounds GS 78 Flexible PVC, Electrical Plugs
Plugs
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DSM Arnite® B600 SNF PBT FR
Flame Retardant
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Barlog Plastics KEBATER BF115 PBT, 15% glass fiber reinforced
PBT-GF15Information provided by BARLOG plastics GmbH.
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological
POM copolymerInformation provided by Celanese
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Celanese Hostaform® C 9021 M XAP2® POM
Description: Injection molding type, modified with molybdenum disulphide; good chemical resistance to solvents, fuel and strong alkalis as well as good hydrolysis resistance; high resistance to ther..
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
DuPont Performance Polymers Delrin® 300CP BK642 Acetal Homopolymer  (Unverified Data**)
Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance. This black is formulated to mainta..
Density 1.42 g/cc
0.0513 lb/in³
ASTM D792
SABIC Innovative Plastics LNP LUBRICOMP DFP34 PC
LNP* Lubricomp* DFP34 is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Internally Lubricated.