Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bostik 6370 Very Flexible EVA Glue Stick

Category Polymer , Adhesive , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Adhesive/Sealant Grade
Manufacturer Bostik
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bostik 6370 Very Flexible EVA Glue Stick.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bostik 6370 Very Flexible EVA Glue StickVery flexible. Bonds wide range of floral, craft and upholstery materials.
Physical Properties Metric English Comments
Viscosity 12000 cP

@Temperature 177 °C
12000 cP

@Temperature 350 °F
Typical
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 60.0 °C
140 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Pot Life 1.0 min
1.0 min
Open Time
Descriptive Properties Value Comments
Color Clear