Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87262 Polyvinyl Chloride, Rigid (PVC, Rigid) The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne |
|||
Flexural Strength | <= 73.0 MPa | <= 10600 psi | ISO 178 |
Polykemi AB POLYabs N20 GF17 ABS, Glass Fiber-Reinforced Information provided by Polykemi AB |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D 790 |
SABIC Innovative Plastics Cycoloy® XCY480 PC+ABS (Europe-Africa-Middle East) High flowThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP Colorcomp D10009 PC (Asia Pacific) LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
Kolon KOCETAL® LW301 Wear Modified Acetal Resin Special polymer added, improved wear property. Applications: Products for low noise and precision gear. Information provided by API-Kolon. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL004 PC (Asia Pacific) LNP* Lubricomp* DL004 is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP IBP34 PA6.12 LNP* LUBRICOMP* IBP34 is a compound based on Nylon 6/12 containing 20% Glass Bead, 15% PTFE/Silicone. Added features include: Wear Resistant. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP QL002 PA 6/10 LNP* LUBRICOMP* QL002 is a compound based on Nylon 6/10 containing 10% PTFE. Added features of this grade are: Wear Resistant. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66 LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing... |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX6601 PPE+PA66 (Asia Pacific) PPE+PA Unfilled GTX |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 1.27 mm/min; ASTM D790 |
SK Chemicals SKYGREEN® PETG 2008 Specially Formulated PET Copolymer Resin SKYGREEN PETG is an amorphous copolyester in which a certain amount of ethylene glycol is replaced with 1,4-cyclohexane dimethanol (CHDM), which prevent crystallization, leading to improved processa.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX6601 PPE+PA66 (Asia Pacific) |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
Plenco 5350 Phenolic, Granular, Injection Molded PLENCO 05350 is a mineral and graphite filled phenolic molding compound, developed for seal applications. PLENCO 05350 offers excellent dimensional stability, lubricity, and low abrasion properties... |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178-93 |
Wellman Wellamid® XT1573-N Impact Modified Nylon 66 Description: Impact Modified Nylon 66Information provided by Wellman. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
Eastman Drystar 0827 Copolyester This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Flexural Strength | 73.0 - 75.0 MPa | 10600 - 10900 psi | ASTM D790M |
DSM Somos® ProtoGen™ 18920 Liquid Photopolymer, UV Postcure Product DescriptionDSM Somos® ProtoGen 18920 is a liquid photopolymer that produces accurate, ABS-like parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demo.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
Denka TE-20 Transparent Resin Polymer (MABS resin) ABS "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 2mm/min; ASTM D790 |
Denka TH-21 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
Denka TP-802 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene "TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 2 mm/min; ISO 178 |
Chi Mei Polylac® PA-727 ABS Electro-plating |
|||
Flexural Strength | 73.0 - 76.0 MPa | 10600 - 11000 psi | ASTM D790 |
3D Systems Accura® ClearVue™ Free (SL 7870) Stereolithography Plastic High clarity plastic for a multitude of applicationsFeaturesClear and transparentRigid and toughGreat for headlamps, bottles and transparent assembliesExcellent humidity/moisture resistanceAll infor.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
Azoty Tarnow™ TARNOFORM 300 GB4 POM 20% glass beads filled grade with increased stiffness and hardness with lowered shrinkageInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
Plenco 2311 Phenolic, Granular, Transfer Molded PLENCO 02311 is a versatile general purpose organic filled phenolic molding compound offering excellent mold processability and optimized cure cycles. PLENCO 02311 is also granulated to provide impr.. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP DL002ER PC (Asia Pacific) LNP* Lubricomp* DL002ER is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Internally Lubricated, Easy Molding, Mold Release. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated. |
|||
Flexural Strength | 73.0 MPa | 10600 psi | ASTM D790 |
SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific) PPE/HIPS for auto interior |